Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 12.5 GPa | 1810 ksi | |
Plastcom SLOVAMID 6 GF 50 TS PA6, 50% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | |
Plastcom SLOVAMID 6/66 GF 50 PA6/66, 50% glass fibre FeaturesPA 6/66 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-g.. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ISO 178, ASTM D790 |
Nilit Nilamid B3 H G8 40% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G8 is a product that combines outstanding strength and stiffness with good moldability and good impact strength. It is widely used for structural applications.Key character.. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DEL34E PC (Asia Pacific) LNP* Lubricomp* DEL34 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 12.5 - 18.6 GPa | 1810 - 2700 ksi | Average value: 15.6 GPa Grade Count:51 |
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi.. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | |
Plastcom SLOVAMID 6 GF 50 LTS PA6, 50% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ASTM D790 |
LATI LARPEEK 50 G/40 40% Glass Reinforced Polyetheretherketone (PEEK)
(discontinued **) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | |
PBI Performance Products Celazole® TF-60 V Glass Fiber Reinforced Melt Processable Polybenzimidazole Celazole® polybenzimidazole (PBI) resin is a unique and highly stable linear hetrocyclic polymer. PBI is characterized by high strength; excellent thermal stability, and broad chemical resistance. .. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP 5CL23 FP-V (PVDF) LNP* LUBRICOMP* 5CL23 is a compound based on PVDF resin containing 15% Carbon Fiber, 10% PTFE. Added features include: Wear Resistant. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ISO 178 |
Hexion Bakelite™ MP 4165 Melamine Phenolic Resin, Copper Adhesive, Low Shrinkage, High Mechanical Strength
(d Melamine/phenolic molding compound, inorganically filled, glass fiber reinforced, good temperature stability, high level of mechanical properties, copper adhesive, flammability UL 94/V-0/1.6 mm (not.. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DF0089 PC LNP THERMOCOMP* DF0089 is a compound based on Polycarbonate resin containing 40% Glass Fiber. Added features include: Flame Retardant. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP LF006E PEEK LNP* THERMOCOMP* LF006E is a compound based on Polyetheretherketone resin containing 30% Glass Fiber. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ISO 178 |
Vyncolit X613 Novolac Phenolic Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties. UL listed.USES: Solenoid covers or automotive under-bonnet applications such as: water pumps, impeller.. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ISO 178 |
Wellman Wellamid® GF43-66 XE-N 43% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data .. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ISO 178-93 |
Wellman Wellamid® MRGF25/25 22H-NBK1 Nylon 66, 25% Mineral and 25% Glass Reinforced All information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ISO 178 |
Polyplastics Duranex® 3400 Polybutylene Terephthalate (PBT), Standard, 40% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | 2 mm/min; ISO 178 |
Eurostar Starflam RF0097P PA66/6, 45% Glass Filled, Injection Molded Starflam RF0097P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1009Z270EM)Information provided by Polym.. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ISO 178 |
Eurotec® Tecodur® PB70 GR50 NL PBT 50% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ISO 178 |
Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, DAM Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass.. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R543H BK02 Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H BK02 is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R543H Black Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Black is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, .. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Dry as Molded Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. .. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 614 Nylon 6, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 624 Nylon 6/6, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.43% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® A-1945 HSL Polyphthalamide (PPA)
(discontinued **) Amodel A-1945 HSL is a 45% glass reinforced grade of polyphthalamide (PPA) resin. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment. Thi.. |
|||
Flexural Modulus | 12.5 GPa | 1810 ksi | ISO 178 |
Solvay Specialty Polymers Ixef® 1313/0004 Polyarylamide, 40% Glass Fiber + Elastomer, DAM
(discontinued **)&l Impact modified. The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manu.. |