Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.34 GPa | 195 ksi | ASTM D790 |
Quadrant EPP Proteus® O & P Grade, Natural Homopolymer Polypropylene (ASTM Product Data Sheet) |
|||
Flexural Modulus | 1.34 GPa | 195 ksi | ASTM D790 |
Quadrant EPP Proteus® PP, Natural Homopolymer Polypropylene (ASTM Product Data Sheet) |
|||
Flexural Modulus | 1.34 GPa | 195 ksi | ASTM D790 |
Polymer Resources NY6/12-GP1 General Purpose Nylon 612 Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Flexural Modulus | 1.34 GPa | 195 ksi | 0.05 in/min; 1% secant; Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CH120 Polypropylene, Homopolymer, Injection Molding, Barefoot Formulated for excellent processing stability. Applications: General purpose injection molding. Equivalent to Pro-fax® HL23INInformation provided by Phillips 66. |
|||
Flexural Modulus | 1.34 GPa | 195 ksi | 0.05 in/min; 1% secant; Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CH200L Polypropylene, Homopolymer, CR, Antistat, Injection Molding COPYLENE™ CH200L is designed for general purpose injection molding applications with anti-static and controlled rheology. Applications: Food Containers, Housewares, Closures.Information provided by.. |
|||
Flexural Modulus | 1.34 GPa | 195 ksi | ASTM D790 |
Quadrant EPP Proteus® PP, ProKnob Finish Natural Homopolymer Polypropylene (ASTM Product Data Sheet) High impact resistance strength Better resistance to cracking at low temperatures than Homopolymer Polypropylene More pliable than homopolymer Meets food handling guidelines Chemical- and corrosion.. |
|||
Flexural Modulus | 1.34 GPa | 195 ksi | ASTM D790 |
Formosa Plastics Formolene® HL5505 Blow Molding HDPE
(discontinued **) Extra High Molecular Weight CopolymerApplications: 55 gallon drums (even those with demanding built-in handling rings), industrial tanksFormolene HL5505 is intended for large part blow molding appli.. |
|||
Flexural Modulus | 1.34 GPa | 195 ksi | ASTM D790 |
Formosa Plastics Formolene® DB5305A Blow Molding HDPE
(discontinued **) Extra High Molecular Weight Polyethylene Formolene® DB5305A is tailored for large part blow molding applications. Besides having excellent chemical resistance properties Formolene® DB5305A HDPE ha.. |
|||
Flexural Modulus | 1.34 GPa | 195 ksi | 0.05 in/min; 1% secant; Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CH050 Polypropylene, Homopolymer, Cast Film BOPP COPYLENE™ CH050 is a polypropylene controlled rheology homopolymer resin designed for Cast Film BOPP (biaxially oriented polypropylene) film extrusion applications. Applications: Bags & Pouches, Pe.. |
|||
Flexural Modulus | 1.34 - 3.17 GPa | 195 - 460 ksi | Average value: 2.27 GPa Grade Count:111 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
Flexural Modulus | 1.34 GPa | 195 ksi | at 0.05 in/min; ASTM D790 |
M. Holland Company CP300 Polypropylene Copolymer Features: Medium Flow, High Impact Resistance, Good StiffnessUses: Appliances, Business, Equipment, Tool/Tote Box, ToysApprovals: FDA 21 CFR 177.1520 Processing Method: Injection MoldingInformatio.. |
|||
Flexural Modulus | 1.34 GPa | 195 ksi | ASTM D790 |
M. Holland Company PP500 Polypropylene Homopolymer Features: Homopolymer, Narrow Molecular Wt. Dist.Uses: Disposable Drinkware, Medical Applications, PackagingApprovals: FDA 21 CFR 177.1520Processing Method: Injection MoldingInformation provided by .. |
|||
Flexural Modulus | 1.34 GPa | 195 ksi | ASTM D790B |
Ineos N02G-00 Polypropylene Impact Copolymer Grade N02G-00 is a low melt flow rate, high-impact copolymer polypropylene for sheet extrusion and thick wall injection molding applications. It offers a superior balance of stiffness and impact str.. |
|||
Flexural Modulus | 1.34 GPa | 195 ksi | ASTM D790 |
LyondellBasell Alathon® L5876 High Density Polyethylene, Blow Molding Grade ALATHON L5876 is designed for injection blow molding and extrusion blow molding applications where higher gloss than standard grades is required. Regulatory Status: L5876 meets the requirements of t.. |
|||
Flexural Modulus | 1.34 GPa | 195 ksi | ASTM D790B |
Ineos N00M-00 Polypropylene Impact Copolymer Grade N00M-00 is a fractional melt flow rate, medium term heat aging, high impact copolymer polypropylene for blow molding, pipe, tubing and sheet extrusion applications. It offers a superior balanc.. |
|||
Flexural Modulus | 1.34 GPa | 195 ksi | ASTM D790 |
Techmer ES HiFill FR® PP FR-N X Availability: North AmericaForms: PelletsFeatures: Flame Retardant Appearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.34 GPa | 195 ksi | ASTM D790 |
Techmer ES HiFill FR® PP FR-N X BKN001 Availability: North AmericaForms: PelletsFeatures: Flame Retardant Appearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.34 GPa | 195 ksi | 1% secant; ASTM D790 |
A. Schulman POLYFORT™ FPP 3391 Chemically Coupled, Modified Polypropylene DescriptionPolyfort® FPP 3391 is a chemically coupled, mineral reinforced high impact resistant, modified polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.34 GPa | 195 ksi | 1% secant; ASTM D790 |
A. Schulman POLYFORT™ FPP 3391 Chemically Coupled, Modified Polypropylene DescriptionPolyfort® FPP 3391 is a chemically coupled, mineral reinforced high impact resistant, modified polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.34 GPa | 195 ksi | 1% Secant; ASTM D790 |
Washington Penn Medium Impact Copolymer 20% Calcium Carbonate Filled Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa.. |
|||
Flexural Modulus | 1.34 GPa | 195 ksi | 1% secant; ASTM D790 |
A. Schulman POLYFORT™ FPP 3391 Chemically Coupled, Modified Polypropylene DescriptionPolyfort® FPP 3391 is a chemically coupled, mineral reinforced high impact resistant, modified polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.34 GPa | 195 ksi | 1% secant; ASTM D790 |
A. Schulman POLYFORT™ FPP 3391 Chemically Coupled, Modified Polypropylene DescriptionPolyfort® FPP 3391 is a chemically coupled, mineral reinforced high impact resistant, modified polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.34 GPa | 195 ksi | 1% secant; ASTM D790 |
A. Schulman POLYFORT™ FPP 3391 Chemically Coupled, Modified Polypropylene DescriptionPolyfort® FPP 3391 is a chemically coupled, mineral reinforced high impact resistant, modified polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.34 GPa | 195 ksi | 1% secant; ASTM D790 |
A. Schulman POLYFORT™ FPP 3391 Chemically Coupled, Modified Polypropylene DescriptionPolyfort® FPP 3391 is a chemically coupled, mineral reinforced high impact resistant, modified polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.34 GPa | 195 ksi | 1% Secant; molded and tested in accordance with ASTM D 4101; ASTM D790A |
Dow C700-35 Polypropylene Resin DOW C700-35 is intended for use in injection molding processes where medium impact strength is required.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braskem in J.. |
|||
Flexural Modulus | 1.34 GPa | 195 ksi | Procedure B, Test Method I(chs 0.05 in/min); ASTM D790 |
Diamond Polymers ASA TWP 502 Description: Transparent Weatherable PolymerInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 1.34 GPa | 195 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem 52T30V Homopolymer Polypropylene Description: Clarified, Excellent Mold Release, Excellent Flow CharacteristicsApplications: Suggested Uses Include Housewares, Storage Boxes, Containers, VialsInformation provided by Braskem |
|||
Flexural Modulus | 1.34 GPa | 195 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem TI4005F Impact copolymer Polypropylene Description: Extra high izod impact, very high flexural modulus, good low temperature drop impact.Applications: Suggested uses include compounding and thermoforming.Process: Thermoforming.This resin.. |