Polymer Property : Flexural Modulus = 2.30 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.0159 GPa
2.30 ksi
ASTM D790
Lubrizol Estane® ALR E77A-V Thermoplastic Polyurethane
Type: Estane® ALR E77A-V is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corp..
Flexural Modulus 0.0159 GPa
2.30 ksi
ASTM D790
Lubrizol Estane® ALR E80A Thermoplastic Polyurethane
Type: Estane® ALR E80A is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Information Provided by The Lubrizol Corporation