Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.48 GPa | 360 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® C1000HF PC+ABS (Asia Pacific) High flow PC+ABS. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® C8080REC PC+ABS PC+ABS Recycle Resin with good flow, good temperature resistance and moderate impact |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | 6.4 mm; ASTM D790 |
SABIC Innovative Plastics FL405 PC Various weight reductions at 0.250"" (6.38 mm) wall. Impact resistant, superior processing, excellent surface. UL94 V-0 at 0.120 |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
Quadrant EPP Ertalyte® TX Internally Lubricated Semi-Crystalline Polyester (ASTM Product Data Sheet) |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
Quantum Modified PPO - Noryl® Information provided by Quantum Advanced Engineering Plastics |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® ML4588 PC Extrusion and extrusion blowmolding grade for aircraft applications. Meets FAR 25.853 (60 seconds/30 mils).This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
M. Holland Company AB308LG ABS Acrylonitrile Butadiene Styrene High flowGood impact resistanceHigh stiffnessApplications: Household goodsPackagingInformation provided by M. Holland |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ISO 178 |
Ineos ABS Lustran® Guardian™ 682 ABS, Injection Molding Grade Lustran® ABS 682 is a high performance, HCFC-141b resistant grade of ABS for injection molded refrigerator and freezer components. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
KYDEX® 152WG Capped Wood Grain Thermoplastic Sheet Features:Super tough, durableHigh extensibility, rigidity, abrasion resistance and fire retardancyMore rigid than most thermoplastics, parts deform less when loadedOutstanding resistance to breakage.. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
KYDEX® XD MB 3D Laminate Thermoplastic 3D Laminate for Flat Lamination and Membrane Pressed Uses with Microban® Features:Tough and extremely durableResistant to cracking and chippingSolid, integral color4,000+ custom colorsResistant to a wide range of chemicalsAbrasion resistantFire retardantVery low moisture.. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
Solvay Specialty Polymers Radel® R-7159 Polyphenylsulfone (PPSU) Radel® R-7159 polyphenylsulfone (PPSU) was developed specifically for aircraft interior applications. The product complies with the FAA regulation 14CFR Part 25 Appendix F, offering vertical burn.. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | secant; ASTM D790 |
Spartech EP5140 Talc Filled Homopolymer Provides the highest level of stiffness and heat resistance of filled olefins. Talc filled grades offer the highest strength properties. Typical applications include extrusion/thermoformed food cont.. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC (Europe-Africa-Middle East) Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP WX05505 PBT LNP* Thermocomp* WX05505 is a compound based on Thermoplastic Polyester (PBT) resin containing proprietary fillers. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6 A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab.. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1453 Calcium Carbonate Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1453 is a long term heat aging grade of 40% calcium carbonate filled homopolymer polypropylene. Information provided by A. Schulman. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN213GL (COND, 50% RH) Nylon 66, 13% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1200 Calcium Carbonate-Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1200 is a 40% calcium carbonate-filled homopolymer polypropylene. Information provided by A. Schulman. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1200 Calcium Carbonate-Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1200 is a 40% calcium carbonate-filled homopolymer polypropylene. Information provided by A. Schulman. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1453 Calcium Carbonate Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1453 is a long term heat aging grade of 40% calcium carbonate filled homopolymer polypropylene. Information provided by A. Schulman. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1453 Calcium Carbonate Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1453 is a long term heat aging grade of 40% calcium carbonate filled homopolymer polypropylene. Information provided by A. Schulman. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
Entec Hylex® P1317FR Polycarbonate Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
Ensinger Tecaform™ Acetal Copolymer - Extruded Products (POM) Tecaform™ is a semi-crystalline thermoplastic offering high strength, stiffness and toughness. It is resistant to hot water, hydrocarbons and solvents, and it posses good bearing and wear properti.. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
Clariant Renol 6602-L Nylon 66, Internally Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
Techmer ES HiFill FR® PA4/6 FR HS Availability: North AmericaForms: PelletsAdditive: Heat StabilizerFeatures: Flame Retardant and Heat StabilizedTPCI# 8277150Information provided by TP Composites, Inc. |