Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.59 GPa | 375 ksi | Tangent; ASTM D790 |
RheTech Products CC40P100-00EG 40% Calcium Carbonate Reinforced Polypropylene, Natural, Extrusion Grade Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | ASTM D790 |
PolyOne Nymax™ 600 A Natural F Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Flexural Modulus | 2.59 GPa | 375 ksi | ASTM D790 |
Polymer Resources TP-FR2 Polybutylene Terephthalate, Flame Retardant Polybutylene Terephthalate, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided.. |
|||
Flexural Modulus | 2.59 GPa | 375 ksi | Tangent; ASTM D790 |
RheTech Products HP506-01A 21% Talc Reinforced High Performance Polypropylene, UV Stabilized, Black Applications: Automotive interior applicationsHVAC ductsTail lamp housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.59 GPa | 375 ksi | ASTM D790 |
PolyOne Lubri-Tech™ SY-000/10T-2S Natural Polystyrene (PS), PTFE Lubricated
(discontinued **) Description/Features:High ImpactPTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | ISO Value |
BASF Capron® 8202 HS BK-102 Nylon 6 (Dry)
(discontinued **) Capron 8202 HS BK-102 is an unfilled, heat stabilized, pigmented black, low viscosity, general purpose nylon 6 exhibiting excellent fluidity for filling thin sections. It possesses the combination.. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | ASTM D790 |
Firestone CR212-203-D Nylon 6, Heat Stabilized Black color. Heat stabilized, Modified, and Lubricated. Chip size is 2 x 3 mm.Information provided by Firestone |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP OL009 PPS - Linear LNP LUBRICOMP* OL009 is a compound based on PPS - Linear resin containing 45% PTFE. Added features of this material include: Wear Resistant. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY AX06484 ABS LNP* STAT-LOY* AX06484 is a compound based on ABS resin containing Talc. Added feature of this grade is: Antistatic, Extrudeable. |
|||
Flexural Modulus | 2.59 GPa | 375 ksi | ASTM D790 |
Techmer ES Plastiblend® PSU CR X Availability: North AmericaForms: PelletsAdditive: TPU Impact Modifier Features: Impact ModifiedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in.. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS (Asia Pacific) Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in.. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON 9X04323 PPE+PA66 (Asia Pacific) LNP* Stat-kon* 9X04323 is a compound based on Noryl GTX resin,Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON RD000IXP PA 66 LNP STAT-KON* RD000IXP is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Flexural Modulus | 2.59 GPa | 375 ksi | 1% Secant; ASTM D790 |
Washington Penn Homopolymer Polypropylene 50% Calcium Carbonate Filled Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa.. |
|||
Flexural Modulus | 2.59 GPa | 375 ksi | ASTM D-790 |
Axiall SP-7221 Rigid PVC, Molding Georgia Gulf SP-7221 is a high impact rigid vinyl compound designed for water distribution systems. The product is NSF listed under Standard 14.Information provided by Georgia GulfGeorgia Gulf beca.. |
|||
Flexural Modulus | >= 2.59 GPa | >= 375 ksi | ASTM D790 |
Buckeye Polymers BP RPP 1209 GR BLK Polypropylene, 12% Glass Filled Product Information: 12% glass reinforced polypropyleneProduct Features:Offers improved flex modulus while maintaining a low specific gravity propertyOffers improved heat stability and scratch and m.. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | ASTM D790 |
PolyOne Lubri-Tech™ MP-000/10T Modified PPO - 10% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Flexural Modulus | 2.59 GPa | 376 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only. |