Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion L1101 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® MG94U ABS High flow, UV stabilized ABS molding grade |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Polymer Resources PC/ABS-FR1-[color]-WR Flame Retardant PC/ABS Alloy, Wear Resistant PC/ABS Alloy, Flame Retardant, Standard Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP COLORCOMP J1000AE PES LNP* COLORCOMP* J1000AE is an unfilled Polyethersulfone. Added feature of this grade is: Easy Molding. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU)
(Unverified Data**) Veradel® PESU was formerly marketed as Gafone™ PESU Veradel 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughn.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
PolyOne Edgetek® AS-1000 Acrylonitrile Butadiene Styrene (ABS)
(discontinued **) Description/Features:UnfilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
BASF Capron® B73QP Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
I. Stern 108B Utility Black ABS Features:Good processing characteristicsInjection Molding and ExtrusionApplicationsProfilesPicture Frames, Tubes, RodsSpools, ReelsInformation provided by I. Stern & Co. Inc. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Techmer ES Electrafil® PC-50/EC Polycarbonate, Conductive Carbon Filled Conductive Carbon, Powder Modified |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 310SE0 PBT (Europe-Africa-Middle East) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Solvay Specialty Polymers Veradel® 3500 Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral ac.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Solvay Specialty Polymers Veradel® A-201 Polyethersulfone (PESU) Veradel® A-201 is a low melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance t.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Solvay Specialty Polymers Veradel® A-301 Polyethersulfone (PESU) Veradel® A-301 is a medium melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability and resistance.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | tangent; ASTM D790 |
Spartech DP5120 Talc Filled Homopolymer Provides the highest level of stiffness and heat resistance of filled olefins. Talc filled grades offer the highest strength properties. Typical applications include extrusion/thermoformed food cont.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® V3504 PBT (Asia Pacific) VALOX EXVX0197 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON RD000I PA 66 (Asia Pacific) LNP* STAT-KON* RD000I is a compound based on Nylon 66 resin containing Carbon Powder, Impact Modifier. Added features of this material include: Electrically Conductive, High Impact. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | 1% Secant; ASTM D790 |
Washington Penn Medium Impact Copolymer 40% Talc Filled Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
BASF Capron® B73ZP Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
PolyOne Edgetek® PF-1000 Polysulfone
(discontinued **) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU)
(Unverified Data**) Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral acids. .. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Techmer ES HiFill FR® PBT FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | Method1, Procedure A (1"x3"x0.125"), Tangent calculation; ASTM D790 |
ExxonMobil Paxon™ BA7718 Sheet Extrusion and Blow Molding Resin
(discontinued **) BA7718 is a 25% brown mica-filled, medium molecular weight, high density polyethylene. This material has been specifically developed as a cost effective resin for applications which require outstan.. |