Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.75 GPa | 399 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
Ovation Polymers SOFTAPLAS™ R 60300 GF Nat Thermoplastic Polyurethane, 30% Glass Fiber 30% short glass fiber reinforced for excellent strength and processabilityAll properties after 48hrs conditioning at 23°C/50% RH |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CX7211 PC+ABS Cycoloy* CX7211 PC/ABS resin is a non-filled, injection moldable grade which has UL 94 rating at 2.5 mm 5VA. Cycoloy CX7211 resin provides all color options and features an excellent balance of flo.. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CX7211 PC+ABS (Asia Pacific) Cycoloy* CX7211 PC/ABS resin is a non-filled, injection moldable grade which has UL 94 rating at 2.5 mm 5VA. Cycoloy CX7211 resin provides all color options and features an excellent balance of flo.. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc.. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS (Asia Pacific) Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc.. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Geloy EXGY30CP ASA Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Geloy FXTW30PE ASA Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Geloy FXW751SK ASA+PC (Europe-Africa-Middle East) Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact ResinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® DMX9254 PC Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl.. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® DMX9254 PC (Europe-Africa-Middle East) Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl.. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® ML7686E PC (Europe-Africa-Middle East) Transparent Polycarbonate in natural color. Excellent processability, super high flow. UL compliant 94V-2 at 1.5mm. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DBP32EI PC LNP* Lubricomp* DBP32EI is a compound based on Polycarbonate resin containing 15% PTFE/Silicone and 10% Glass Bead. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.75 GPa @Thickness 3.20 mm |
398 ksi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical PI642G ABS, General Purpose, High Modulus Feature: Extrusion Molding, General Purpose, High ModulusApplication: Pipe fittingCAS No. 9003-56-9Information provided by LG Chemical |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DZL34E PC (Asia Pacific) LNP* Lubricomp* DZL34E is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer LNP* LUBRICOMP* KG002 is a compound based on Acetal Copolymer resin containing 10% Graphite. Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP QAP22S PA6.10 LNP* LUBRICOMP* QAP22S is a compound based on Nylon 6/10 resin containing 10% PTFE/Silicone, 10% Aramid Fiber. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP ZI001XXX PPE+PS (Asia Pacific) LNP* Lubricomp* ZI001XXX is a compound based on PPE+PS Blend resin. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY U2000A PPA LNP* LUBRILOY* U2000A is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DX03550 PC LNP STAT-KON* DX03550 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DX03550 PC (Asia Pacific) LNP STAT-KON* DX03550 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp FF008L PE LNP* Thermocomp* FF008L is a compounding based on Polyethylene containing glass fiber. Added characteristics include Low Extractible.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.75 GPa | 398 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NE-1010 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM 9085 PEI Blend (Asia Pacific) High flow Polyetherimide blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke and flame evolution. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® FXV310SK PBT VALOX FXV310SK is an unreinforced PBT injection moulding Visualfx* resin with high flow characteristics and containing a metal sparkle. Applications: automotive bezels and appliances. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | 15mm/min; ASTM D790 |
Denka MALECCA K-400 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Flexural Modulus | 2.75 GPa @Thickness 3.20 mm |
398 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SP 6605 Toughened Polystyrene Characteristics Excellent melt strength High stiffness Easy tearability Processing Extrusion Applications Suitable for thin film for candy wrap and window envelope Economic production of clear th.. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics GELOY FXW751SK ASA+PC Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact Resin |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DBL349E PC LNP* Lubricomp* DBL349E is a compound based on Polycarbonate resin containing 20% Glass Bead, 15% PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retard.. |