Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 2030 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 11.0 - 14.0 GPa
1600 - 2030 ksi
Injection; ISO 178
Raschig Group 5562 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
Flexural Modulus 11.0 - 14.0 GPa
1600 - 2030 ksi
Compression; ISO 178
Raschig Group DECAL® 572R Phenolic
Glass-fiber reinforced phenolic molding compound. Exceptional heat resistance with regard to maintaining surface finish and mechanical properties, outstanding mechanical properties, excellent rotati..
Flexural Modulus 2.41 - 14.0 GPa
350 - 2030 ksi
Average value: 4.13 GPa Grade Count:47
Overview of materials for Polyetheretherketone, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values..
Flexural Modulus 5.00 - 14.0 GPa

@Temperature -40.0 - 121 °C
725 - 2030 ksi

@Temperature -40.0 - 250 °F
Average value: 8.45 GPa Grade Count:8
Overview of materials for Nylon 66, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. ..
Flexural Modulus 12.0 - 14.0 GPa
1740 - 2030 ksi
ISO 178
Vyncolit G885 Novolac Phenolic
Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties. Information provided by Vyncolit, a Sumitomo Bak Group
Flexural Modulus 12.0 - 14.0 GPa
1740 - 2030 ksi
ISO 178
Vyncolit X658 Novolac Phenolic
Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties and a very good dimensional stability.USES: Complex precision parts.Information provided by ..
Flexural Modulus 10.0 - 14.0 GPa
1450 - 2030 ksi
ISO 178
Bulk Molding Compounds tetra-DUR L 4305 Bulk Molding Compound
UL-licensed. Anchor wave-isolation.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion prote..
Flexural Modulus 10.0 - 14.0 GPa
1450 - 2030 ksi
ISO 178
Bulk Molding Compounds tetra-DUR N 4303 Bulk Molding Compound
Mechanical high grade standard product.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion p..
Flexural Modulus 11.0 - 14.0 GPa
1600 - 2030 ksi
ISO 178
Vyncolit X682 Novolac Phenolic
Glass fiber, glass bead and graphite filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction.USES: Water pump seals and self-lubricating bearings.Info..
Flexural Modulus 12.0 - 14.0 GPa
1740 - 2030 ksi
Injection; ISO 178
Raschig Group DECAL® 152CL Phenolic
Glass-fiber and mineral reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meet..
Copyright © lookpolymers.com All Rights Reserved