Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.41 - 14.5 GPa | 350 - 2100 ksi | Average value: 4.72 GPa Grade Count:21 |
Overview of materials for Polycarbonate, Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Conductive". Each property range of values reported is minimum and maximum values of appr.. |
|||
Flexural Modulus | 10.5 - 14.5 GPa | 1520 - 2100 ksi | Average value: 11.9 GPa Grade Count:12 |
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an.. |
|||
Flexural Modulus | 11.7 - 14.5 GPa | 1700 - 2100 ksi | |
Bulk Molding Compounds BMC 1000 Thermoset Polyester, Food Grade BMC 1000 is a general purpose, food contact grade, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. As with all other BMC, Inc. compounds, .. |
|||
Flexural Modulus | 11.7 - 14.5 GPa | 1700 - 2100 ksi | |
Bulk Molding Compounds BMC 1100 Corelyn Glass Fiber Reinforced Polyester Compound BMC 1100, also known as CoreLyn, is a food contact safe material with excellent scratch and stain resistant properties. CoreLyn can be pigmented to match virtually any color. This glass fiber-reinfo.. |
|||
Flexural Modulus | 12.4 - 14.5 GPa | 1800 - 2100 ksi | |
Bulk Molding Compounds BMC 700 Thermoset Polyester, High Arc Quench Electrical Grade BMC 700 is a general purpose, mineral filled, glass fiber-reinforced polyester compound that was initially designed for molding arc chutes. It has superior arc quench properties. As with all other B.. |
|||
Flexural Modulus | 7.52 - 14.5 GPa | 1090 - 2100 ksi | Average value: 10.7 GPa Grade Count:10 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |