Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 15.1 GPa | 2190 ksi | (102 mm Span) 3mm/min; ASTM D790 |
LNP ULTEM® UC3000 Polyetherimide, 30% Carbon Fiber Reinforcement
(discontinued **) High modulus with shielding/ conductive characteristics for high-heat applications.Features: Electrically Conductive, High Heat Resistance, High StrengthForms: PelletsProcessing Method: Injection Mo.. |
|||
Flexural Modulus | 15.1 GPa | 2190 ksi | d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 50 000000 Nylon 6, Glass Fiber Reinforced PA 6, 50% glass fibers, injection moldingInformation provided by LANXESS. |
|||
Flexural Modulus | 15.1 GPa | 2190 ksi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621.. |
|||
Flexural Modulus | 15.1 GPa | 2190 ksi | ASTM D790 |
Sumitomo Bakelite North America Epiall® 1908-1 Short Glass Fiber Reinforced Epoxy Epiall 1908-1 is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation proper-ties that meets the requir.. |
|||
Flexural Modulus | 15.1 GPa | 2190 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp OC004 PPS - Linear (Europe-Africa-Middle East) LNP* THERMOCOMP* OC004 is a compound based on PPS-Linear resin containing Carbon Fiber. Added features include : Electrically Conductive.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |
|||
Flexural Modulus | 15.1 GPa | 2190 ksi | ASTM D790 |
Plenco 6015 Phenolic, Briquette, Transfer Molded PLENCO 06015 is a glass and mineral filled phenolic molding compound offering improved mechanical strength, dimensional stability and excellent electrical properties. 06015 is available in black.Inf.. |
|||
Flexural Modulus | 15.1 GPa | 2190 ksi | 2 mm/min; ISO 178 |
Eurostar Starglas OC004 PPS, 20% Carbon Filled, Injection Molded Starglas OC004 is a 20% Carbon Fiber Reinforced PPS Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 15.1 GPa | 2190 ksi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621 CF30 gr.. |
|||
Flexural Modulus | 15.1 GPa | 2190 ksi | ASTM D790 |
Quantum Composites QC-8151C 55% Glass Fiber Vinyl Ester Static-Dissipative SMC
(discontinued **) QC-8151C is a vinyl ester sheet molding compound (SMC) designed for compression molding components requiring dimensional stability, resistance to high temperatures plus sufficient electrical conduct.. |
|||
Flexural Modulus | 15.1 GPa | 2190 ksi | (102 mm Span) 3mm/min; ASTM D790 |
LNP ULTEM® SMU5836 Polyetherimide, 30% Carbon Fiber Reinforcement
(discontinued **) High modulus with shielding/ conductive characteristics for high-heat applications.Features: Electrically Conductive, High Heat Resistance, High StrengthForms: PelletsProcessing Method: Injection Mo.. |