Mechanical Properties Metric English Comments
Flexural Modulus 15.9 GPa
2310 ksi
ASTM D790
PolyOne Gravi-Tech™ GRV-NY-112-W-NAT Polyamide 6 (Nylon 6)
Information provided by PolyOne
Flexural Modulus 15.9 GPa

@Temperature 23.0 °C
2310 ksi

@Temperature 73.4 °F
ISO 178
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep ..
Flexural Modulus 15.9 GPa
2310 ksi
(50.8 mm Span) 1mm/min; ASTM D790
LNP ULTEM® EXCP0096 Polyetherimide, 30% Carbon Fiber Reinforcement, 10% PTFE Lubricant  (discontinued **)
Features: Lubricated, Electrically Conductive, Good Wear Resistance, High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This dat..
Flexural Modulus 15.9 GPa

@Temperature 23.0 °C
2310 ksi

@Temperature 73.4 °F
ISO 178
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry)
Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr..
Flexural Modulus 15.9 GPa
2310 ksi
ISO 178
Solvay Specialty Polymers Kalix® 9950 Polyamide, High Performance (HPPA), 50% Glass Fiber
Kalix® 9950 is a 50% glass-fiber reinforced high-performance polyamide. It is hot-water moldable and intended for use in components requiring superior mechanical properties and excellent surface ..
Flexural Modulus 15.9 GPa
2310 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP EC006 PEI (Europe-Africa-Middle East)
LNP* THERMOCOMP* EC006 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features include: Electrically Conductive.
Flexural Modulus 15.9 GPa
2310 ksi
ASTM D790
Sumitomo Bakelite North America Epiall® 1908B-1 Short Glass Fiber Reinforced Epoxy
Epiall 1908B-1 is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation properties.Information provided ..
Flexural Modulus 15.9 GPa
2310 ksi
ASTM D790
Sumitomo Bakelite North America Epiall® 2061B-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy
Epiall 2061B-1 is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by S..
Flexural Modulus 15.9 GPa
2310 ksi
ASTM D790
Plenco 7556 Phenolic, Briquette, Transfer Molded
PLENCO 07556 is a glass fiber reinforced novolac phenolic molding compound, with good physical strengths and heat resistance along with excellent dimensional stability. UL recognized under component..
Flexural Modulus 15.9 GPa
2310 ksi
ASTM D790
Sumitomo Bakelite North America RX® 647 Fiberglass Reinforced Phenolic
RX 643 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-10. RX 647 is a fibe..
Flexural Modulus 15.9 GPa
2310 ksi
ASTM D790
Sumitomo Bakelite North America RX® 853G Fiberglass Reinforced Phenolic Novolac
RX 853G is a fiberglass reinforced phenolic novolac compound, featuring dimensional stability, moderate impact resistance, and good strength and modulus.Information supplied by Sumitomo Bak North Am..
Flexural Modulus 15.9 GPa
2310 ksi
ASTM D790
A. Schulman ComAlloy Hiloy® 716 PPS, Carbon Fiber Reinforced
Data provided by the manufacturer, ComAlloy International Company.20% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.