Mechanical Properties Metric English Comments
Flexural Modulus 1.66 GPa
241 ksi
Ineos Styrenics Polystyrene 476M Q598 (NAFTA)
High-impact grade of polystyrene with good ESCR designed to provide uniform melt flow for excellent processability.Information provided by BASF.Ineos Styrenics purchased this product line from BASF ..
Flexural Modulus 1.66 GPa
241 ksi
1% secant; ASTM D790-02
Ipiranga Petrochem PH 0133 Polypropylene
The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr..
Flexural Modulus 1.66 GPa
241 ksi
1% secant; ASTM D790-02
Ipiranga Petrochem PH 0133 Polypropylene
The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr..
Flexural Modulus 1.66 GPa
241 ksi
1% secant; ASTM D790-02
Ipiranga Petrochem PH 1721 Polypropylene
The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr..
Flexural Modulus 1.66 GPa
241 ksi
1% secant; ASTM D790-02
Ipiranga Petrochem PH 1721 Polypropylene
The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr..
Flexural Modulus 1.66 GPa
241 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON MD000A PP
LNP* STAT-KON* MD000A is a compound based on Polypropylene resin containing Carbon. Added feature of this grade is: Electrically Conductive.
Flexural Modulus 1.66 GPa
241 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON MD000AP PP
LNP* STAT-KON* MD000AP is a compound based on Polypropylene containing Carbon Powder. Added features of this grade include: Electrically Conductive, Exceptional Processing.
Flexural Modulus 1.66 GPa
241 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Xenoy® 5720U PBT+PC
Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY
Flexural Modulus 1.66 GPa
241 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Asia Pacific)
Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY
Flexural Modulus 1.66 GPa
241 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East)
Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY
Flexural Modulus 1.66 GPa
241 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Stat-kon TE002
LNP* Stat-kon* TE002 is a compound based on Polyurethane resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the A..
Flexural Modulus 1.66 GPa
241 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON TE002 PU
LNP* STAT-KON* TE002 is a compound based on Polyurethane resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive.
Flexural Modulus 1.66 GPa
241 ksi
ASTM D 790
SABIC Innovative Plastics LNP Stat-loy 9X05426C PMMA
LNP* Stat-loy* 9X05426C is a compound based on PMMA resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 1.66 GPa
241 ksi
ASTM D 790
SABIC Innovative Plastics LNP Stat-loy 9X05426C PMMA (Asia Pacific)
LNP* Stat-loy* 9X05426C is a compound based on PMMA resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 1.66 GPa
241 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-LOY A3000LTH ABS
LNP* STAT-LOY* A3000LTH is a compound based on ABS resin. Added features of this material include: Transparent, Antistatic, Formulation Locked.
Flexural Modulus 1.66 GPa
241 ksi
ASTM D 790
SABIC Innovative Plastics LNP Stat-loy K3000 Acetal Copoly
LNP* Stat-loy* K3000 is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americas regi..
Flexural Modulus 1.66 GPa
241 ksi
ASTM D 790
SABIC Innovative Plastics LNP Stat-loy K3000 Acetal Copoly (Asia Pacific)
LNP* Stat-loy* K3000 is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Asia Pacific ..
Flexural Modulus 1.66 GPa
241 ksi
ASTM Test
Styrolution Luran® S 776 SE ASA
Luran S 776 SE is a general purpose extrusion ASA grade with good toughness and strength, used for sheet and profile extrusions.Information provided by STYROLUTION, which is a joint venture between ..
Flexural Modulus 1.66 GPa
241 ksi
ASTM D790
Samsung Cheil Industries Starex® WR-9750 Extrusion Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Flexural Modulus 1.66 GPa
241 ksi
ASTM D790
Samsung Cheil Industries Starex® WR-9750 Extrusion Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Flexural Modulus 1.66 GPa
241 ksi
ASTM Test
BASF Ultraform N 2640 Z4 UNC Q600 POM
Ultraform N2640 Z4 UNC Q600 is a high toughness, elastomer-modified injection molding POM grade.