Mechanical Properties Metric English Comments
Flexural Modulus 1.379 - 1.792 GPa
200.0 - 259.9 ksi
ASTM D790
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
Flexural Modulus 1.379 - 1.792 GPa
200.0 - 259.9 ksi
ASTM D790
Arkema Group KYNAR® 460 Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Broad molecular weight distribution, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, ..