Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.24 GPa | 470 ksi | Tangent; ASTM D790 |
RheTech Products M40P200-01 40% Mica Reinforced Polypropylene Copolymer, Black Applications: Automotive applicationsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | |
Quadrant EPP Ertalon® 66 SA PA 66, extruded (ISO Data) Material with a higher mechanical strength, stiffness, heat and wear resistance than Ertalon 6 SA. It also has a better creep resistance but its impact strength and mechanical damping ability is red.. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Polymer Resources PEI-GP1-TFE5 Polyetherimide, 5% PTFE, Flame Retardant Polyetherimide, General Purpose, 5% PTFE, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Ineos Nova 1210 High Heat Crystal Polystyrene
(discontinued **) High heat resistance, High molecular weight, optimum performance in extruded foamApplications: Meat and poultry trays, Egg cartons, Food packagingExposure to gamma radiation in the 2.02-6.06 megarad.. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Ineos Nova 1230 High Heat Crystal Polystyrene
(discontinued **) Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r.. |
|||
Flexural Modulus | 3.24 - 10.9 GPa | 470 - 1580 ksi | Average value: 7.78 GPa Grade Count:62 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM Data |
BASF Capron® 5202 HS BK-102 Nylon 66 (Dry)
(discontinued **) Capron 5202 HS BK-102 is an unfilled, heat stabilized, pigmented black nylon 6,6, injection molding compound. It combines strength and stiffness as well as excellent chemical resistance. The additi.. |
|||
Flexural Modulus | 3.24 GPa | 469 ksi | ASTM D790 |
Lendell Parapet PMMA, High Flow |
|||
Flexural Modulus | 3.24 GPa @Thickness 3.20 mm |
469 ksi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical GPPS 20HR(E) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
Flexural Modulus | 3.24 GPa @Thickness 3.20 mm |
469 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® LW5102F PBT+PC+GF10% Description: Injection Molding, PBT+PC+GF10%, Low Warpage, Flame RetardantApplication: IT/OA, E&E (Switch)CAS No. 9003-01-04, 68928-70-1, 65997-17-3, 24968-12-5, 103598-77-2 and 1309-64-4Information.. |
|||
Flexural Modulus | 3.24 GPa @Thickness 3.20 mm |
469 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GP2102 PC+GF10% Description: Injection Molding, PC+GF10%, General Purpose, Good Toughness, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790-1 |
Ineos Styrenics 158K High-Heat Polystyrene Crystal Resin (Global) Description: High-heat, high-molecular weight grades for a variety of applications, including medical devices and labware, cosmetics packaging, CD & DVD jewel boxes, food serviceware, and low-taste,.. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
LG Chemical LUPOL GP-3154F General Purpose Polypropylene, 15% Mineral Fillers, High Modulus, Flame Retardant LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 9075 PEI High flow Polyetherimide blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF10 IM L BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight Additive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Com.. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF7 L 7% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 7% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Techmer ES HiFill® POM HO UV Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: HomopolymerInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.24 GPa | 469 ksi | ASTM D790 |
Samyang Tribit® 1500G15K PBT, Reinforced Impact Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1500G15K is a reinforced, impact grade.Appl.. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Chase Plastics CP Pryme® PC310R Polycarbonate, 10% Glass Fiber Reinforced, Recycled Content Features: Good mold releaseRecycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Videolar 585 Crystal Polystyrene (GPPS) High heat extrusion crystalSuperior oriented polystyrene sheetFeatures: Low melt flowHigh molecular weightApplications: Foam applications such as egg cartons, meat trays and food serviceSuperior ori.. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Chesterton ARC 982 100% Novolac acid resistant coating Description: An advanced polymer composite formulated to protect equipment from extreme chemical attack and corrosion. A low viscosity composite that is applied by brush, squeegee, or a plural compo.. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM Test |
BASF Ultramid® 1310-11 NF2001 PA66 (Dry) Ultramid 1310-11 NF2001 is a controlled crystallization, fast cycling PA6/6 which provides extremely fast cycle times and improved productivity over Ultramid 1000. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Americas Styrenics EA3130 High Heat Crystal Polystyrene Product CharacteristicsAdditive FreeFood Contact CompliantTypical ApplicationsMedical PartsColor Concentrate CarrierLow Profile AdditivesInformation provided by AmericasStyrenics LLC. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Americas Styrenics EA3400 High Heat Crystal Polystyrene Product CharacteristicsLess than 300 parts per million residual volatiles with minimal taste and odor transferExcellent clarity and colorGood toughnessFood Contact CompliantTypical ApplicationsCap l.. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Americas Styrenics STYRON® 685D High Heat Crystal Polystyrene Product CharacteristicsHigh heat resistanceHigh tensile strengthBlue tintFood Contact CompliantUL Classification 94HBUSP Class VITypical ApplicationsFoamOPSMedicalInformation provided by AmericasSty.. |
|||
Flexural Modulus | 3.24 GPa | 469 ksi | ASTM D790 |
Cheng Yu Plastic E500G20 PC/PET, 20% Glass Fiber |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Asahi Kasei Thermylene® P6-20FG-0754 20% Glass, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Ineos Nova 1220 High Heat Crystal Polystyrene
(discontinued **) Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r.. |