Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.50 GPa @Temperature 23.0 °C |
508 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANFILL Injection CPC35051 PP/PE, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 3.50 GPa @Temperature 23.0 °C |
508 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANTEC PC S60R GF10 Polycarbonate, Glass-Fiber Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 3.50 GPa | 508 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® 505RU PC (Asia Pacific) Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro.. |
|||
Flexural Modulus | 3.50 GPa | 508 ksi | |
Plastcom SLOVASTER® B GB 30 PBT, 30% glass beads FeaturesPBT for injection moulding, chemically reinforced with 30% glass beads. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Flexural Modulus | 3.50 GPa | 508 ksi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-820 SL10 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL10 is a polyetheretherketone (PEEK) based compound designed to offer enhanced lubricity and reduced friction compared to standard PEEK. Unlike other grades formulated for wear res.. |
|||
Flexural Modulus | 3.50 - 20.7 GPa | 508 - 3000 ksi | Average value: 7.28 GPa Grade Count:22 |
Overview of materials for Polyphenylene Sulfide (PPS), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Aramid Fiber". Each property range of values reported is minimum and maximu.. |
|||
Flexural Modulus | 3.50 GPa | 508 ksi | |
Lehmann & Voss LUVOCOM® 1301-7932 PPS, linear, with aramid reinforcement and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage, isotropic shrinkage .. |
|||
Flexural Modulus | 3.50 GPa | 508 ksi | 2 mm/min; ISO 178 |
Inno-Comp INNOPOL® CS 1-3820 20% Glass-Fiber-Filled Polypropylene Homopolymer INNOPOL® CS 1-3820 is a 20% glass-fiber-filled polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-3820 is recommended for producing in.. |
|||
Flexural Modulus | 3.50 GPa | 508 ksi | ASTM D790 |
Loxim 110 01V0 Polycarbonate, 10% Glass Filled, Flame Retardant Information provided by Loxim Industries |
|||
Flexural Modulus | 3.50 GPa | 508 ksi | |
Lehmann & Voss LUVOCOM® 1100-7725 VP Polyether sulfone, with glass fiber, lubricant modified Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Flexural Modulus | 3.50 GPa | 508 ksi | |
Lehmann & Voss LUVOCOM® 1105/GR/15/TF/15-2 PEEK, with PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,.. |
|||
Flexural Modulus | 3.50 GPa | 508 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RAL22 PA 66 (Asia Pacific) LNP LUBRICOMP* RAL22 is a compound based on Nylon 66 resin containing Aramid, PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 3.50 GPa | 508 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 (Asia Pacific) LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing Aramid Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 3.50 GPa | 508 ksi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-820 SL10 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL10 is a polyetheretherketone (PEEK) based compound designed to offer enhanced lubricity and reduced friction compared to standard PEEK. Unlike other grades formulated for wear.. |
|||
Flexural Modulus | 3.50 GPa | 508 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® 4012G PBT VALOX 4012G is a 10% glass fiber reinforced PBT injection molding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility. |
|||
Flexural Modulus | 3.50 GPa | 508 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Flexural Modulus | 3.50 GPa | 508 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DZ004 PC LNP* Thermocomp* DZ004 is a compound based on Polycarbonate resin containing 20% Milled Glass. |
|||
Flexural Modulus | 3.50 GPa | 508 ksi | 2 mm/min; ISO 178 |
Sax Polymers SAXAMID 226K6 Nylon 6.6, 30% Glass Beads SAXAMID 226K6 is a polyamide 6.6 injection-molding-grade filled with 30% glass beads. It is characterized by optimized shrinkage properties.Information provided by SAX Polymers |
|||
Flexural Modulus | 3.50 GPa | 508 ksi | ASTM D 790 |
SABIC Innovative Plastics Noryl HS2000 PPE (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 3.50 GPa | 508 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GFN1 PPE+HIPS (Europe-Africa-Middle East) NORYL GFN1 is a standard 10 % glass fibre reinforced material with a HDT/A of 110C according ISO 75. NORYL GFN1 can be used for all applications where a higher modulus is required. NORYL GFN1 is ava.. |
|||
Flexural Modulus | 3.50 GPa | 508 ksi | ASTM D790 |
Unitika AX-1500W Dry Characteristics: A resin succeeding the advantages of AX1500 resin and containing titanium oxide at high concentration. Improved drastically in light reflection and blocking properties, aimed at dis.. |
|||
Flexural Modulus | 3.50 GPa | 508 ksi | ISO 178 |
Polyram RamOfin PPH501G4 Polypropylene, 20% Glass Fiber, Flame Retardant Glass fiber 20% reinforced, halogen free, flame retardant polypropylene for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 3.50 GPa | 508 ksi | ISO 178 |
Polyplastics Duracon® TR-10D Acetal Co-polymer (POM), Mineral filling, Mineral filling, High rigidity, Low warpage DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Flexural Modulus | 3.50 GPa | 508 ksi | ASTM-D790 |
Polyram PlusTek PB847I4 Nylon 6, 20% Glass Fiber and Mineral 20% glass fiber and mineral reinforced, impact modified polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 3.50 GPa | 508 ksi | ASTM D790, ISO 178 |
EPICHEM Epilen PP 20GF NAT Polypropylene, 20% Glass Fiber Characteristics: 20% glass fibre filled |
|||
Flexural Modulus | 3.50 GPa | 508 ksi | ISO 178 |
Eurostar Star L PA66 D91 PA66, Aramid Fiber Filled, Injection Molded Star L PA66 D91 is a PTFE lubricated, Aramid Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 3.50 GPa | 508 ksi | ASTM D790 |
E-Polymers TEKANATE™ G710 , 10% Glass Fiber Reinforced Poly Carbonate 10% Glass Fiber reinforcedInformation provided by E-Polymers Co. Ltd. |
|||
Flexural Modulus | 3.50 GPa | 508 ksi | |
Asahi Kasei Xyron® NC42Z Modified Polyphenylene Ether Applications: Automotive: Door Handles, Fuse Carriers, Fuse Box Covers, Interior Electrical Outlets, Interior Plugs/Switches, Interior High Precision Parts Electrical and Industrial: Pool and Spa P.. |
|||
Flexural Modulus | 3.50 GPa | 508 ksi | ASTM D790 |
Gharda Chemicals GATONE™ 5300PF Polyetheretherketone (PEEK)
(discontinued **) Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric.. |
|||
Flexural Modulus | 3.50 GPa | 508 ksi | ASTM D790 |
LATI LASTIROL TR G/10-V1 10% Glass Fiber Reinforced Polystyrene (PS) (UL94 V-1)
(discontinued **) Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |