Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.585 GPa | 520.0 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1007X Extra High Flow, Talc Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1007X is an extra high flow, 40% talc fortified homopolymer polypropylene. Information provided by A. Schulman. |
|||
Flexural Modulus | 3.585 GPa | 520.0 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 809 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 809 is a 40% talc-filled homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.585 GPa | 520.0 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 809 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 809 is a 40% talc-filled homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.585 GPa | 520.0 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1007X Extra High Flow, Talc Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1007X is an extra high flow, 40% talc fortified homopolymer polypropylene. Information provided by A. Schulman. |
|||
Flexural Modulus | 3.585 GPa | 520.0 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 809 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 809 is a 40% talc-filled homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.585 GPa | 520.0 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 809 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 809 is a 40% talc-filled homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.585 GPa | 520.0 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1007X Extra High Flow, Talc Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1007X is an extra high flow, 40% talc fortified homopolymer polypropylene. Information provided by A. Schulman. |
|||
Flexural Modulus | 3.585 GPa | 520.0 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 809 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 809 is a 40% talc-filled homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.585 GPa | 520.0 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1007X Extra High Flow, Talc Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1007X is an extra high flow, 40% talc fortified homopolymer polypropylene. Information provided by A. Schulman. |
|||
Flexural Modulus | 3.585 GPa | 520.0 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 809 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 809 is a 40% talc-filled homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 3.585 GPa | 520.0 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1007X Extra High Flow, Talc Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1007X is an extra high flow, 40% talc fortified homopolymer polypropylene. Information provided by A. Schulman. |
|||
Flexural Modulus | 3.585 GPa | 520.0 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1007X Extra High Flow, Talc Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1007X is an extra high flow, 40% talc fortified homopolymer polypropylene. Information provided by A. Schulman. |