Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 35.0 GPa | 5080 ksi | |
Lehmann & Voss LUVOCOM® 1115/XCF/40 PEK, with carbon fiber Applications: High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts, non flammable.Electrically c.. |
|||
Flexural Modulus | 35.0 GPa | 5080 ksi | |
Saint-Gobain Quartzel® Fiber/Epoxy Resin Unidirectional Composite Quartzel® fiber is produced from quartz crystal that is ground, purified, fiberized by a fusion process. It is homogeneous, non-porous, continuous, amorphous, ultra pure silica glass. It is of.. |
|||
Flexural Modulus | 35.0 GPa | 5080 ksi | 0° |
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, E-glass UD fabric 315 g/m2 Information provided by HexCel |
|||
Flexural Modulus | 35.0 GPa | 5080 ksi | 0° |
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, E-glass UD fabric 430 g/m2 Information provided by HexCel |
|||
Flexural Modulus | 35.0 GPa | 5080 ksi | 0° |
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, Hybrid carbon/Aramid fabric 245 g/m2 Information provided by HexCel |
|||
Flexural Modulus | 35.0 GPa | 5080 ksi | transverse; ISO 178 |
Bond Laminates TEPEX® dynalite 408-C200(2)-FG290(4)/45% Carbon – Filament Glass – TPU Consolidated Composite Laminate Within the TEPEX® composite laminate, TPU distinguishes itself from alternative resin systems by its specific physical properties. The TPU resin is tough which results in an excellent impact and f.. |