Mechanical Properties Metric English Comments
Flexural Modulus 2.59 GPa
376 ksi
ASTM D790
PolyOne Maxxam™ DP-8928-2-1000 Polypropylene, Unspecified (PP, Unspecified)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Flexural Modulus 2.59 GPa
376 ksi
ASTM D790
PolyOne Maxxam™ DP-8928-2-8001 Polypropylene, Unspecified (PP, Unspecified)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Flexural Modulus 2.59 GPa
376 ksi
ASTM D790
PolyOne Nymax™ 600 A Natural F Polyamide 6 Alloy (Nylon 6 Alloy)
The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials..
Flexural Modulus 2.59 GPa
376 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS (Asia Pacific)
CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only.
Flexural Modulus 2.59 GPa
376 ksi
ASTM D790
PTS Trilac® ABS-HS4000 General Purpose ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
Flexural Modulus 2.59 GPa
376 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® ML6451 PC
UV-stabilized, co-extrusion capstock material. Minimal processing values available at this time.
Flexural Modulus 2.59 GPa
376 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® ML6451 PC (Asia Pacific)
UV-stabilized, co-extrusion capstock material. Minimal processing values available at this time.
Flexural Modulus 2.59 GPa
376 ksi
ASTM D790
PolyOne Lubri-Tech™ SY-000/05T High Impact Styrene - 5% PTFE  (discontinued **)
Data provided by PolyOne.
Flexural Modulus 2.59 GPa
376 ksi
ISO Value
BASF Capron® 8202 HS BK-102 Nylon 6 (Dry)  (discontinued **)
Capron 8202 HS BK-102 is an unfilled, heat stabilized, pigmented black, low viscosity, general purpose nylon 6 exhibiting excellent fluidity for filling thin sections. It possesses the combination..
Flexural Modulus 2.59 GPa
376 ksi
ASTM D790
Firestone C212-15C Nylon 6, Heat Stabilized
Off white color. Heat stabilized, Modified, and Lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone
Flexural Modulus 2.59 GPa
376 ksi
ASTM D790
Firestone CR212-203-D Nylon 6, Heat Stabilized
Black color. Heat stabilized, Modified, and Lubricated. Chip size is 2 x 3 mm.Information provided by Firestone
Flexural Modulus 2.59 GPa
376 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP OL009 PPS - Linear
LNP LUBRICOMP* OL009 is a compound based on PPS - Linear resin containing 45% PTFE. Added features of this material include: Wear Resistant.
Flexural Modulus 2.59 GPa
376 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP OL009 PPS - Linear (Asia Pacific)
LNP* LUBRICOMP* OL009 is a compound based on PPS - Linear resin containing PTFE. Added features of this material include: Internally Lubricated.
Flexural Modulus 2.59 GPa
376 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DX05305C PC (Asia Pacific)
LNP* Stat-kon* DX05305C is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Clean Compounding System.
Flexural Modulus 2.59 GPa
376 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Stat-kon RX89129 PA 66
LNP* Stat-Kon RX89129 is a compound based on Nylon 6,6. Fillers are proprietary.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.59 GPa
376 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-LOY AX06484 ABS
LNP* STAT-LOY* AX06484 is a compound based on ABS resin containing Talc. Added feature of this grade is: Antistatic, Extrudeable.
Flexural Modulus 2.59 GPa
376 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Stat-loy AX06484X ABS
LNP* Stat-Loy* AX06484 is a compound based on ABS resin containing mineral filler. Characteristics of this grade is it is extrudeable and static dissipative.This data was supplied by SABIC-IP for t..
Flexural Modulus 2.59 GPa
376 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS
Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in..
Flexural Modulus 2.59 GPa
376 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS (Asia Pacific)
Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in..
Flexural Modulus 2.59 GPa
376 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS (Europe-Africa-Middle East)
Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in..
Flexural Modulus 2.59 GPa
376 ksi
ASTM D790
SABIC Innovative Plastics NORYL PPO534 PPE+HIPS (Asia Pacific)
PPO/PS unfilled high heat
Flexural Modulus 2.59 GPa
376 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL PX500 PPE (Asia Pacific)
Noryl PX500 is an unfilled modified polyphenylene ether resin capable of multiple conversion routes. This resin is designed for lower odor during conversion than many standard modified PPE resins. ..
Flexural Modulus 2.59 GPa
376 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON 9X04323 PPE+PA66 (Asia Pacific)
LNP* Stat-kon* 9X04323 is a compound based on Noryl GTX resin,Added features of this material include: Electrically Conductive.
Flexural Modulus 2.59 GPa
376 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DX05305C PC
LNP* STAT-KON* DX05305C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System.
Flexural Modulus 2.59 GPa
376 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON RD000IXP PA 66
LNP STAT-KON* RD000IXP is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Flexural Modulus 2.59 GPa
376 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP AB002 ABS
LNP* THERMOCOMP* AB002 is a compound based on ABS resin containing 10% Glass Bead.
Flexural Modulus 2.59 GPa
376 ksi
ASTM D790
PolyOne Lubri-Tech™ MP-000/10T Modified PPO - 10% PTFE  (discontinued **)
Data provided by PolyOne.
Flexural Modulus 2.59 GPa
376 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS
CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only.