Polymer Property : Flexural Modulus = 39.2 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.270 GPa
39.2 ksi
1.7 mm/min; DIN 53457
Advanced Elastomer Systems VistaFlex® 912-B Thermoplastic Rubber  (discontinued **)
Description: A black super high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as ..
Flexural Modulus 0.270 GPa
39.2 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP YP003 POLYESTER ELASTOMER
LNP LUBRICOMP* YP003 is a compound based on Polyester Elastomer resin containing 15% PTFE/Silicone. Added features of this material include: Wear Resistant.
Flexural Modulus 0.270 GPa
39.2 ksi
ISO 178
SABIC Innovative Plastics LNP Lubricomp YP003 TPEE
LNP LUBRICOMP* YP003 is a compound based on TPEE resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas ..
Flexural Modulus 0.270 GPa
39.2 ksi
Tangent - 16:1 span:depth, 0.5 in/min; ASTM D-790
Chevron Phillips Marlex® C101 Polyethylene; Enhanced
Metallocene linear low density polyethylene. This linear low density, hexene copolymer is tailored for blow molded containers that require: High glossGood clarityExcellent ESCR Applications: Typi..
Flexural Modulus 0.270 GPa
39.2 ksi
Conditioned 15 days at 23°C - 50% RH; ISO 178
Arkema Group Pebax® MV 1041 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® MV 1041 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This hydrophilic grade when extruded into either a thin film or laminated on ..
Flexural Modulus 0.270 GPa
39.2 ksi
ASTM D790
C.O.I.M. LARIPUR® LPR5850 Modified Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
Flexural Modulus 0.270 GPa

@Temperature 65.0 °C
39.2 ksi

@Temperature 149 °F
ASTM Test
BASF Ultramid® 8350 HS PA6 (Dry)
Ultramid 8350 HS is a heat stabilized, impact modified type 6 graft copolymer developed for extrusion, tubing, and jacketing applications requiring a high level of toughness combined with a moderate..