Mechanical Properties Metric English Comments
Flexural Modulus 2.69 GPa
390 ksi
ASTM D790
PolyOne Geon™ Vinyl Packaging JGR 136A Clear 13FG Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Flexural Modulus 2.69 GPa
390 ksi
ASTM D790
PolyOne Geon™ Vinyl Packaging VB7 White 215 Polyvinyl Chloride, Rigid (PVC, Rigid)
A rigid PVC Compound designed for extrusion blow molding balusters for railings.Information provided by PolyOne
Flexural Modulus 2.69 GPa
390 ksi
ASTM D790
PolyOne Geon™ Vinyl Rigid Molding MR200 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Flexural Modulus 2.69 GPa
390 ksi
ASTM D790
PolyOne Nanoblend™ LST 5501 Polypropylene, Unspecified (PP, Unspecified)
Nanoblend compounds, formerly known as Maxxam LST, are LIGHT, STIFF AND TOUGH. Using nanoclay technology, these compounds deliver a combination of high stiffness and impact resistance to meet demand..
Flexural Modulus 2.69 GPa
390 ksi
Tangent; ASTM D790
RheTech Products T28P100-01EG 28% Talc Reinforced Polypropylene, Black, Extrusion Grade
Applications: Window trimConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 2.69 GPa
390 ksi
Test Method I, Procedure B (chs speed 0.05 in/min), Tangent; ASTM D790
Network Polymers NPP 30-0200 TF20
Description: 20% Talc Filled Homopolymer PolypropyleneInformation provided by Network Polymers Inc.
Flexural Modulus 2.69 GPa
390 ksi
ASTM D790
Quantum Polysulfone
Information provided by Quantum Advanced Engineering Plastics
Flexural Modulus 2.69 GPa

@Thickness 3.17 mm
390 ksi

@Thickness 0.125 in
ASTM D790
PTS PCA-2201NH Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Flexural Modulus 2.69 GPa
390 ksi
ASTM D790
Solvay Specialty Polymers Udel® P-1700 Polysulfone (PSU)  (Unverified Data**)
Udel P-1700 polysulfone (PSU) is a tough, rigid, high-strength thermoplastics suitable for continuous use up to 300°F (149°C). It is resistant to oxidation and hydrolysis and withstand prolonged e..
Flexural Modulus 2.69 GPa
390 ksi
ASTM D790
Solvay Specialty Polymers Udel® P-1750 MR Polysulfone (PSU)  (Unverified Data**)
Udel P-1750 MR is a lower color grade of polysulfone that contains a mold release which aids part ejection when parts with low draft are injection molded. Polysulfones have long been known for trans..
Flexural Modulus 2.69 GPa
390 ksi
ASTM D790
Solvay Specialty Polymers Udel® P-3500 LCD Polysulfone (PSU)  (Unverified Data**)
Udel P-3500 LCD is a very high molecular weight grade of polysulfone, and therefore offers the greatest toughness and chemical resistance of the available grades. It is well-suited for extrusion. Th..
Flexural Modulus 2.69 GPa
390 ksi
Molded; ASTM D790
Honeywell Aegisâ„¢ H135MP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H135MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR..
Flexural Modulus 2.69 GPa
390 ksi
ASTM-D790
Ineos ABS Lustran® ABS 349
Lustran® ABS 349 is a high-gloss, medium-impact injection molding resin that has been specially formulated for excellent surface lubricity using internal additives.
Flexural Modulus 2.69 GPa
390 ksi
ASTM D 790
MRC Polymers NAXALOYâ„¢ 793MF6 PC + Polyester Blend, 6% Mineral Filled
• Available in natural and custom colors• Can be UV Stabilized• Internal and external lubricants can be addedInformation provided by MRC Polymers Inc.
Flexural Modulus 2.69 GPa
390 ksi
ASTM D790
Solvay Specialty Polymers Udel® P-1710 Polysulfone (PSU)
Udel® P-1710 polysulfone (PSU) is a tough, rigid, high-strength thermoplastic that is suitable for continuous use up to 300°F (149°C). The resin is resistant to oxidation and hydrolysis and..
Flexural Modulus 2.69 GPa
390 ksi
ASTM D790
Solvay Specialty Polymers Udel® P-1750 MR Polysulfone (PSU)
Udel® P-1750 MR is a lower color grade of polysulfone that contains a mold release which aids part ejection when parts with low draft are injection molded.Polysulfones have long been known for tr..
Flexural Modulus 2.69 GPa
390 ksi
ASTM D790
Solvay Specialty Polymers Udel® P-3500 LCD MB Polysulfone (PSU)
Udel® polysulfone is a tough, rigid, high-strength thermoplastic with outstanding hydrolytic resistance. Udel® P-3500 LCD MB series polymers are particularly well suited for the fabrication of..
Flexural Modulus 2.69 GPa
390 ksi
ASTM D790
Solvay Specialty Polymers Udel® P-3500 LCD Polysulfone (PSU)
Udel® P-3500 LCD is a very high molecular weight grade of polysulfone, and therefore offers the greatest toughness and chemical resistance of the available grades. It is well-suited for extrusion..
Flexural Modulus 2.69 GPa
390 ksi
ASTM D790
Techmer ES HiFill® PBT HS BK
Availability: North AmericaForms: PelletsAdditive: Heat StabilizerFeatures: Good Flow, Good Processability and Heat StabilizedAppearance: BlackInformation provided by TP Composites, Inc.
Flexural Modulus 2.69 GPa
390 ksi
ASTM D790
Techmer ES Luriblend® PA6 TL10 Nylon 6
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (10%)Features: Heat Stabilized and LubricatedAppearance: BlackInformation provided by TP Composites, Inc.
Flexural Modulus 2.69 GPa
390 ksi
ASTM D790
Techmer ES Plastiblend® PC/ABS FR 1950 BK
Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc.
Flexural Modulus 2.69 GPa
390 ksi
ASTM D790
Solvay Specialty Polymers Udel® P-1700 Polysulfone (PSU)
Udel® P-1700 polysulfone (PSU) is a tough, rigid, high-strength thermoplastics suitable for continuous use up to 300°F (149°C). It is resistant to oxidation and hydrolysis and withstand pro..
Flexural Modulus 2.69 GPa

@Thickness 3.20 mm
390 ksi

@Thickness 0.126 in
Injection Molded; ASTM D790
Styron EMERGEâ„¢ 7700 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
Overview: EMERGEâ„¢ PC/ABS 7700 Advanced Resin is an ignition-resistant PC/ABS blend that contains no chlorine for bromine additives. It has superior processability for injection molding applicat..
Flexural Modulus 2.69 GPa
390 ksi
ASTM D790
Techmer ES Plastiblend® ABS LE WT
Availability: North AmericaForms: PelletsFeatures: Low Extractables and Medium Impact ResistanceAppearance: WhiteInformation provided by TP Composites, Inc.
Flexural Modulus 2.69 GPa

@Temperature 22.8 °C
390 ksi

@Temperature 73.0 °F
ASTM D790
Ensinger HYDEX® 4101L Polybutylene Terephthalate (PBT)
HYDEX® 4101 & 4101L (lubricated) is a very stable chemical compound that can withstand high impact without deterioration. It is approved for direct contact with food by the FDA and is ideal for ma..
Flexural Modulus 2.69 GPa
390 ksi
ASTM D790
Clariant Renol 6601L Nylon 66, Lubricated
Data provided by Clariant Masterbatches
Flexural Modulus 2.69 GPa
390 ksi
ASTM D-790
Axiall ProTherm® 4529 CPVC Rigid PVC, Molding
Georgia Gulf ProTherm® 4529 CPVC is a pelletized injection molding compound designed for large fittings. Typical applications are in potable water and chemical transfer systems especially where hi..