Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.50 GPa | 653 ksi | ASTM D790 |
Niche Polymer PA66MI40BK Nylon 66, 40% Mineral Fiber Filled, Impact Modified Information provided by Niche Polymer |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | ISO 178 |
Radici Radilon® ACP300 K (dry) Nylon 66 Heat stabilized mineral filledInformation provided by Radici group. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | ISO 178/1A |
Radici Raditer® B RV 150 Polybutylene Terephthalate with 15% Glass fiber Raditer® B RV 150 is a glass fiber reinforced thermoplastic polyester based on polybutylene terephthalate. The PBT compounds combine excellent thermal, mechanical, electrical and chemical properti.. |
|||
Flexural Modulus | 4.50 GPa @Temperature 90.0 °C |
653 ksi @Temperature 194 °F |
ISO 178, ASTM D790 |
Nilit Nilamid A3 H6 G5 25% Glass Reinforced PA66 Description: Nilamid A3 H6 G5 is a 25% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat.. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP BX05029 SAN (Europe-Africa-Middle East) LNP* Lubricomp* BX05029 is a compound based on Styrene Acrylonitrile resin containing Mineral, Graphite. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | ASTM D790 |
PolyOne Edgetek® NJ-10GF/000 Nylon 12 - 10% Glass Fiber
(discontinued **) Data provided by PolyOne. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | |
Lehmann & Voss LUVOCOM® 20/AF/15/TF/10 Polyphthalamide, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low influence from moisture an.. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | Tangent at 0.05 in/min; ASTM D790A |
LyondellBasell Higlass PF072-2 Polypropylene Homopolymer, 20% Glass Fiber Key Features: conventional melt flow, medium high modulus, chemically coupled, glass fiber-reinforced polypropylene homopolymer, moderately high rigidity, high strength, good impact resistanceApplic.. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL SE1GFN2 PPE+HIPS (Europe-Africa-Middle East) Noryl* SE1GFN2 is a 20% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non.. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | 2 mm/min, 64mm span; ISO 178 |
SABIC Innovative Plastics SABIC PPCOMPOUND G3220A PP SABIC® PPcompound G3220A is a general purpose, 20% glass filled, chemically coupled, heat stabilized homopolymer polypropylene compound. The IMDS is 209767996. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM HU2100 PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. For medical devices and pharmaceutical applications.Healthcare management of change, biocom.. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM HU2100 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. For medical devices and pharmaceutical applications.Healthcare management of change, biocom.. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM PW2100 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Specific grade-colors are designed and certified for use in Potable Water applications. KTW, WRAS, ACS, NSF-61 and W270 certified... |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 815F PBT+PET PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 815F PBT+PET (Europe-Africa-Middle East) PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® DR51 PBT (Europe-Africa-Middle East) VALOX DR51 is a 15% glass fiber reinforced PBT injection moulding resin with excellent mechanical, thermal and electrical performance. Applications: spotlights, appliance housings, handles. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP MF741XXH PP LNP* THERMOCOMP* MF741XXH is a compound based on Polypropylene reain containing Glass Fiber and proprietay antimicrobial additives. Designed for touch surfaces in patient critical healthcare applic.. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GFN2 PPE+HIPS (Europe-Africa-Middle East) NORYL GFN2 is a standard 20 % glass fibre reinforced material with a HDT/A of 130C according ISO 75. NORYL GFN2 can be used for all applications where a higher modulus is required. NORYL GFN2 is ava.. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 815F PBT+PET (Asia Pacific) PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1606 Glass Filled Chemically Coupled Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1606 is a 30% glass filled chemically coupled impact copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | ISO 178 |
Unitika M1030DH PA6, Dry Nano composite nylonInformation provided by Unitika Ltd. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | ISO 178 |
Polyram PlusTek PA355M6 Nylon 6.6 for Injection Molding, 30% Mineral Filled, Flame Retardant 30% Minerals filled, flame retardant Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | ISO 178 |
Polyram PlusTek PA350M6 Nylon 6.6 for Injection Molding, 30% Mineral Reinforced 30% Minerals Reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | ISO 178 |
Eurostar Starglas FF006 HDPE, Glass Fiber Filled Starglas FF004 is a Glass Fiber Reinforced High Density Polyethylene Resin (also known as Starglas PE HE 30V)Information provided by Eurostar. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | ISO 178 |
Eurotec® Tecodur® PB70 GR20 NL IH PBT 20% glass fiber reinforced, impact modified Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | ISO 178 |
Cossa Polimeri ESTABLEND PA 1050 GF HI ABS / Nylon 6 Blend, 25% Glass Filled ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.25% glass fiber reinforcedHigh impact strength, high chemical resistance, excellent heat resistance, high dimensional stabi.. |
|||
Flexural Modulus | 4.50 GPa @Temperature 23.0 °C |
653 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPH T5060 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 4.50 GPa | 653 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R860 BK02 Nylon 66, Glass/Mineral Reinforced, Conditioned Vydyne® R860 BK02 is general-purpose, glass-fiber and mineral-reinforced PA66 resin. Available in black, this product is also lubricated for improved flow and offers superior surface appearance. Gl.. |