Polymer Property : Flexural Modulus = 42.1 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.290 - 12.9 GPa
42.1 - 1880 ksi
Average value: 2.60 GPa Grade Count:723
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Flexural Modulus 0.290 GPa
42.1 ksi
ASTM D790
ExxonMobil Iotek® 8610 Sodium Ionomer  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A low melt index sodium ionomer made from an ethylene acrylic acid base polymer. It is designed to have high durability, resilience and impact stre..
Flexural Modulus 0.290 GPa
42.1 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP YL003C Polyester Elastomer
LUBRICOMP* YL003C is a compound based on Polyester Elastomer resin containing 15% PTFE. Added features of this grade include: Clean Compound System, Wear Resistant.
Flexural Modulus 0.290 GPa
42.1 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP YL003C Polyester Elastomer (Asia Pacific)
LUBRICOMP* YL-4030 CCS is a PTFE Lubricated Compound based on Polyester Elastomer resin which has low ionic and low outgassing performance for the Semicon and Internal Hard Disk Drive applications.
Flexural Modulus 0.290 GPa
42.1 ksi
ASTM D790
Sterigenics Raprex® R-300 Branched Linear Low Density Polyethylene
Applications: Foam and ExtrusionRAPREX® R-300 is a linear low density polyethylene based resin that exhibits an excellent balance of melt processability and physical properties due to its unique ..
Flexural Modulus 0.290 GPa
42.1 ksi
ASTM D790
Sterigenics Raprex® R300D Branched Linear Low Density Polyethylene
Applications: Foam and ExtrusionRAPREX® R300D is a linear low density polyethylene based resin that exhibits an excellent balance of melt processability and physical properties due to its unique ..
Flexural Modulus 0.290 GPa
42.1 ksi
ASTM D790
Teknor Apex Telcar® TL-1000-92 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec..
Flexural Modulus 0.290 GPa
42.1 ksi
ASTM D790
Teknor Apex Telcar® TL-1000-92-UV Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec..
Flexural Modulus 0.290 GPa
42.1 ksi
ASTM D790
Toyobo PELPRENE™ S2004FS Polyester TPE, Flame Resistant
Features: Polyester TPE, Flame ResistantInformation provided by Toyobo.
Flexural Modulus 0.290 GPa
42.1 ksi
ISO 178
DuPont Performance Polymers Hytrel® HTR8730 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Viscosity Polyester Elastomer with Excellent Mechanical Properties at Elevated Temperatures Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Flexural Modulus 0.290 GPa
42.1 ksi
ASTM D790
Arkema Group Pebax® 6333 Polyether Block Amide (PEBA)
Information provided by Arkema Group