Mechanical Properties Metric English Comments
Flexural Modulus 2.94 GPa
427 ksi
ASTM D790
Omni Plastics OmniTuff™ HPP TF20 Homopolymer Polypropylene Talc Filled
Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni..
Flexural Modulus 2.94 GPa
427 ksi
ASTM D790
I. Stern GPPS-020 General Purpose Crystal Polystyrene
Features:High Strength GradeHigh Flow, High ToughnessExcellent ProcessabilityApplicationsInjection MoldingAgency RatingsFDA Title 21 CFR 177.1640UL File E185934Information provided by I. Stern & Co...
Flexural Modulus 2.94 GPa

@Thickness 6.40 mm
427 ksi

@Thickness 0.252 in
15mm/min; ASTM D790
LG Chemical LUCON CP6052 PC/ABS+CNT
Description Injection Molding Grade, PC/ABS+CNT, Electrostatic Dissipation, Low Surface Resistivity, Improved Impact StrengthApplication: Laser diode Tray, ATM parts, Telecommunication Station Housi..
Flexural Modulus 2.94 GPa
427 ksi
DIN 53452; ASTM D790
Kolon KOPA® KN126 General Purpose Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Flexural Modulus 2.94 GPa

@Thickness 3.20 mm
427 ksi

@Thickness 0.126 in
1.3mm/min; ASTM D790
LG Chemical LUMAX GP5106FI PBT+ABS+GF10%, Flame Retardant
Description: Injection Molding Grade, PBT+ABS+GF10%, Flame Retardant, Impact Modified, Dimensional StabilityApplication: E&E (Switch)CAS: 9003-56-9, 68928-70-1, 65997-17-3, 24968-12-5, 9003-54-7 an..
Flexural Modulus 2.94 GPa
427 ksi
DIN 53452; ASTM D790
Kolon KOPA® KN136 General Purpose Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Flexural Modulus 2.94 GPa
427 ksi
DIN 53452; ASTM D790
Kolon KOPA® KN3311 General Purpose Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin..
Flexural Modulus 2.94 GPa

@Thickness 6.40 mm
427 ksi

@Thickness 0.252 in
1.3mm/min; ASTM D790
LG Chemical LUPOL HI2202B PP+GF20%, High Impact
Description: Injection Molding, PP+GF20%, General Purpose, High ImpactApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0, 65997-17-3 and 9010-79-1Information provided by LG Chemica..
Flexural Modulus 2.94 GPa
427 ksi
DIN 53452; ASTM D790
Kolon KOPA® KN132VO Flame Retardant Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Flexural Modulus 2.94 GPa
427 ksi
DIN 53452; ASTM D790
Kolon KOPA® KN171 General Purpose Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Flexural Modulus 2.94 GPa
427 ksi
DIN 53452; ASTM D790
Kolon KOPA® KN3311N General Purpose Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin..
Flexural Modulus 2.94 GPa
427 ksi
Shinil Chemical SHINSTAT MS Electrostatic Control Polymer Injection Grade
SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for ..
Flexural Modulus 2.94 GPa
427 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Infino® CF-3104HF PC, 10% Glass Filled High Impact
High-impact PC/GR material for the exterior of slim mobile phoneInformation provided by Samsung Cheil Industries.
Flexural Modulus 2.94 GPa
427 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Infino® CF-3104HF PC, 10% Glass Filled High Impact
High-impact PC/GR material for the exterior of slim mobile phoneInformation provided by Samsung Cheil Industries.
Flexural Modulus 2.94 GPa

@Thickness 3.20 mm
427 ksi

@Thickness 0.126 in
ASTM D790
Supreme Petrochem SC 201E General Purpose Polystyrene
CharacteristicsVery high molecular weight High heat grade Good melt strength Good clarity and mechanical strengthProcessing Extrusion MoldingApplicationsExtruded embossed sheets, OPS, foamed meat t..
Flexural Modulus 2.94 GPa

@Thickness 3.20 mm
427 ksi

@Thickness 0.126 in
ASTM D790
Supreme Petrochem SC 208 General Purpose Polystyrene
CharacteristicsHigh flow grade Easy processing Good clarity & shineProcessing Extrusion MoldingApplications Hand molding applications of novelty items, toys etc. Carrier for master batches, as a ..
Flexural Modulus 2.94 GPa

@Thickness 3.20 mm
427 ksi

@Thickness 0.126 in
ASTM D790
Supreme Petrochem SP201 4551 Light Stabilized Polystyrene
Characteristics Excellent light stability to fluorescent & incandescent light sources Very high clarity and heat resistance Excellent strength & stiffness Processing Injection molding Extrusion A..