Polymer Property : Flexural Modulus = 46.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.317 GPa
46.0 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Eastman M3019-P Polyethylene  (discontinued **)
M3019-P is suggested for applications such as spiral-wound can linings, release paper, and photographic paper. M3019-P Has been found to exhibit good barrier properties, temperature resistance, and..
Flexural Modulus 0.317 GPa
46.0 ksi
at 1% secant modulus; ASTM D790
A. Schulman CP808-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 808-01 is a lineal low-density polyethylene having good processability and exceptional toughness in injection molded parts. This compound has excellent flexibility, high impact streng..
Flexural Modulus 0.317 GPa
46.0 ksi
at 1% secant modulus; ASTM D790
A. Schulman CP814-01 Linear, Low-Density Polyethylene
DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA ..
Flexural Modulus 0.317 GPa

@Temperature -20.0 °C
46.0 ksi

@Temperature -4.00 °F
ASTM D790
DuPont Elvax® 660 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
Flexural Modulus 0.317 GPa
46.0 ksi
at 1% secant modulus; ASTM D790
A. Schulman CP808-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 808-01 is a lineal low-density polyethylene having good processability and exceptional toughness in injection molded parts. This compound has excellent flexibility, high impact streng..
Flexural Modulus 0.317 GPa
46.0 ksi
at 1% secant modulus; ASTM D790
A. Schulman CP814-01 Linear, Low-Density Polyethylene
DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA ..
Flexural Modulus 0.317 GPa
46.0 ksi
at 1% secant modulus; ASTM D790
A. Schulman CP808-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 808-01 is a lineal low-density polyethylene having good processability and exceptional toughness in injection molded parts. This compound has excellent flexibility, high impact streng..
Flexural Modulus 0.317 GPa
46.0 ksi
at 1% secant modulus; ASTM D790
A. Schulman CP808-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 808-01 is a lineal low-density polyethylene having good processability and exceptional toughness in injection molded parts. This compound has excellent flexibility, high impact streng..
Flexural Modulus 0.317 GPa
46.0 ksi
at 1% secant modulus; ASTM D790
A. Schulman CP814-01 Linear, Low-Density Polyethylene
DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA ..
Flexural Modulus 0.317 GPa
46.0 ksi
at 1% secant modulus; ASTM D790
A. Schulman CP808-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 808-01 is a lineal low-density polyethylene having good processability and exceptional toughness in injection molded parts. This compound has excellent flexibility, high impact streng..
Flexural Modulus 0.317 GPa
46.0 ksi
at 1% secant modulus; ASTM D790
A. Schulman CP814-01 Linear, Low-Density Polyethylene
DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA ..
Flexural Modulus 0.317 GPa
46.0 ksi
ASTM D790
Lubrizol Estane® ALR E65D Thermoplastic Polyurethane
Type: Estane® ALR E65D is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corpor..
Flexural Modulus 0.317 GPa
46.0 ksi
at 1% secant modulus; ASTM D790
A. Schulman CP808-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 808-01 is a lineal low-density polyethylene having good processability and exceptional toughness in injection molded parts. This compound has excellent flexibility, high impact streng..
Flexural Modulus 0.317 GPa
46.0 ksi
at 1% secant modulus; ASTM D790
A. Schulman CP814-01 Linear, Low-Density Polyethylene
DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA ..
Flexural Modulus 0.317 GPa
46.0 ksi
at 1% secant modulus; ASTM D790
A. Schulman CP814-01 Linear, Low-Density Polyethylene
DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA ..
Flexural Modulus 0.317 GPa
46.0 ksi
Dow DOWLEX™ 2517 Linear Low Density Polyethylene, Narrow MW Distribution
DOWLEX® 2517 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent environmental stress crack resistance and low temperature properties with excellent f..
Flexural Modulus 0.317 - 0.931 GPa
46.0 - 135 ksi
Average value: 0.630 GPa Grade Count:67
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Rotational Molded
This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Rotational Molded". Each property range of values reported i..