Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.45 GPa | 790 ksi | |
Plastcom SLOVALEN PH 49 GF 25 PP, 25% glass fibre, mod. of mech. properties FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 25 % glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Flexural Modulus | 5.45 GPa | 790 ksi | Tangent; ASTM D790 |
RheTech Products F25-01 34% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Support ductsHousingsBattery traysArm rest insertsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 5.45 GPa | 790 ksi | Tangent; ASTM D790 |
RheTech Products F35-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Interior trimUnderhood componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 5.45 GPa | 790 ksi | after 16 hours in 50°C water |
Malvern Minerals Thermoplastic Polyester with Novacite® 1250 Quartz Filler Product data demonstrates the effect of the Novacite (untreated lamellar quartz) filler. A separate entry demonstrates the effect of surface-treated Novakup filler in thermoplastic polyester Th.. |
|||
Flexural Modulus | 5.45 GPa | 790 ksi | ASTM D790 |
Techmer ES Electrablend® PA6/6 GF13 SS10 BK 13/10% Glass/Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber/Stainless Steel Reinforcement, 13/10% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Appearance: BlackInformation.. |
|||
Flexural Modulus | 5.45 GPa | 790 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP WH0200B PBT LNP* Thermocomp* WH0200B is a compound based on PBT resin containing proprietary fillers. Added features include: High Specific Gravity. |
|||
Flexural Modulus | 5.45 GPa | 790 ksi | Tangent; ASTM D790 |
Plastics Group Polifil® GFPPCC-30 30% Glass Reinforced Polypropylene Polifil® GFPPCC series compounds are homopolymer polypropylenes reinforced with chemically coupled glass fibers. These compounds offer superior strength and stiffness, improved elevated temperature.. |
|||
Flexural Modulus | 5.45 GPa | 790 ksi | ASTM D790 |
Chesterton ARC S2 Ceramic reinforced erosion resistant coating Description: An advanced ceramic composite for the resurfacing and protection of all metal surfaces. It is normally applied at a thickness of 250 microns (10 mils) per coat. Non-shrinking, 100% soli.. |
|||
Flexural Modulus | 5.45 GPa | 790 ksi | ASTM D790 |
Chesterton MRS S2 Metal Rebuilding System An advanced ceramic composite for the resurfacing and protection of all metal surfaces. It is normally applied at a thickness of 250 microns (10 mils) per coat. Non-shrinking, 100% solids. MRS S2 is.. |
|||
Flexural Modulus | 5.45 GPa | 790 ksi | ASTM D790, ISO 178 |
EPICHEM Epilac R ABS 17% GF ABS, 17% Glass Fiber Characteristics: 17% glass fibre filled |
|||
Flexural Modulus | 5.45 GPa | 790 ksi | ASTM D790 |
Asahi Kasei Thermylene® P7-30FG-0684 30% Glass Fiber Reinforced, Heat and UV Stabilized Information provided by Asahi Thermofil |