Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.72 GPa | 540 ksi | Tangent; ASTM D790 |
RheTech Products GC20P200-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural Applications: Consumer goodsBoat handlesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | ASTM D790 |
PolyOne Maxxam™ PD 40 TF Black Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | ASTM D790 |
PolyOne Nymax™ GB 1200 30 HS BLACK 18 Polyamide 66 (Nylon 66) Preliminary Data SheetMolded Test Bars: Dry as MoldedInformation provided by PolyOne |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | Tangent; ASTM D790 |
RheTech Products M30P100-01 30% Mica Reinforced Polypropylene, Black Applications: Fan shroudsHVAC ductworkClose-out panelsFiller panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | ASTM D790 |
Polymer Resources NY66-IMG13-[color]H Nylon, 13% Glass Reinforced, Impact Modified, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | Secant; ASTM D790 |
Fiberfil® J-60/20/E/NS Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled, NSF listed Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Modulus | 3.73 GPa @Thickness 3.20 mm |
540 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOS GP2100 ABS+GF10%, General Purpose Feature: Injection Molding, ABS+GF10%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Modulus | 3.73 GPa @Temperature 23.0 °C |
540 ksi @Temperature 73.4 °F |
ASTM D790 |
IRPC Polimaxx Polene 121PC Styrene Acrylonitrile APPLICATIONS: INJECTION MOLDING, HOUSEHOLD PRODUCTS : SANITARY WARE, AUTOPART APPLICATION : LAMP ELECTRICAL APPLIANCES : ELECTRICAL FAN |
|||
Flexural Modulus | 3.73 GPa @Temperature 23.0 °C |
540 ksi @Temperature 73.4 °F |
ASTM D790 |
IRPC Polimaxx Polene 129PC Styrene Acrylonitrile APPLICATIONS: INJECTION MOLDING, HOUSEHOLD PRODUCTS : SANITARY WARE, AUTOPART APPLICATION : LAMP, ELECTRICAL APPLIANCES : ELECTRICAL FAN |
|||
Flexural Modulus | 3.73 GPa @Temperature 23.0 °C |
540 ksi @Temperature 73.4 °F |
ASTM D790 |
IRPC Polimaxx Polene 320PC Styrene Acrylonitrile APPLICATIONS: INJECTION MOLDING, HOUSEHOLD PRODUCTS : SANITARY WARE, AUTOPART APPLICATION : LAMP ELECTRICAL APPLIANCES : ELECTRICAL FAN |
|||
Flexural Modulus | 3.73 GPa @Temperature 23.0 °C |
540 ksi @Temperature 73.4 °F |
ASTM D790 |
IRPC Polimaxx Polene 330PC Styrene Acrylonitrile APPLICATIONS: INJECTION MOLDING, HOUSEHOLD PRODUCTS : SANITARY WARE, AUTOPART APPLICATION : LAMP ELECTRICAL APPLIANCES : ELECTRICAL FAN |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP KFP032 Acetal Copolymer (Asia Pacific) LNP* LUBRICOMP* KFP032 is a compound based on Acetal Copolymer resin containing PTFE, Silicone, Glass Fiber. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RAL229 PA 66 LNP* LUBRICOMP* RAL229 is a compound based on Nylon 66 containing 10% Aramid, 10% PTFE. Added features of this grade include: Flame Retardant, Wear Resistant. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1100EF PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1100EF PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 1100F PEI Standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA and EU Food Contact compliant. UL94 V0, V2 and 5VA listing. Effective June 2007, this grade will no longer be supported with biocompa.. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 1110 PEI Enhanced flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 1110 PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1110R PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU1110 PEI Enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | 2.6 mm/min, 100 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem MD130A PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | 2.6 mm/min, 100 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem MD131A PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 3.73 GPa | 540 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NH-1150HH PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 3.73 GPa | 540 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® LS-3104G PC, 10% Glass Filled High Impact High-impact resistant PC/GF with 10% GF reinforcement for LCD BLFInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | ASTM D790 |
TPI Porene® AS 121 PC (Blue) General Purpose SAN Porene® is a registered trademark of Thai Petrochemical Industry Co. LTD. Information provided by Dayson Polymers. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | ASTM D790 |
Chesterton ARC PW Potable Water Coating Description: ARC PW is a 100% solids lining certified for NSF/ANSI 61 potable water, cold water service. It is recommended to be applied by brush, roll or spray at 500-750 microns (20-30 mils) total.. |
|||
Flexural Modulus | 3.72 GPa @Temperature 23.0 °C |
540 ksi @Temperature 73.4 °F |
DAM; ASTM D790 |
DuPont Performance Polymers Minlon® EFE6096 GY090A Nylon 66
(Unverified Data**) Minlon® EFE6096 GY090A is a 15% mineral reinforced impact modified nylon 66 resin.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | >= 3.72 GPa | >= 540 ksi | ASTM D790 |
Arlon AD350A PTFE/Woven Fiberglass/Ceramic Filled Composite Tighter Dielectric Tolerance Low Z-Axis Thermal ExpansionCeramic Filled PTFEHigh Thermal ConductivityLarge Panel SizeBenefits:Higher Consistency of PerformanceSuperior PTH AdhesionHeat Dissipation a.. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | ASTM D790 |
Teknor Apex Chemlon® 109-18 GH Nylon 66, 18% Glass Fiber Reinforced Notes: High-impact; Reinforced with 18% glass fibers; Highly toughened compound designed to improve practical toughness and ductility Features: Ductile; Good Impact Resistance; Good Toughness; Good .. |
|||
Flexural Modulus | 3.72 GPa | 540 ksi | ASTM D790 |
PlastxWorld CEVIAN®-N 080 SAN resin These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |