Mechanical Properties Metric English Comments
Flexural Modulus 0.379 GPa
55.0 ksi
ASTM D790
M. Holland Company LL700 LLDPE  (discontinued **)
Features: High ESCR (Stress Crack Resist.), Good Flexibility, High FlowUses: Closures, Household GoodsProcessing Method: Injection MoldingInformation provided by M. Holland.
Flexural Modulus 0.379 GPa
55.0 ksi
Tangent, 0.05 in/min; ASTM D790
LyondellBasell Hifaxâ„¢ CA138A Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ CA138A low modulus thermoplastic olefin (TPO) resin is designed for impact modification and injection molding applications. It is based on material produced from Basell'..
Flexural Modulus 0.379 GPa
55.0 ksi
ASTM D790
Teknor Apex Telcar® TL-1000-105 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Flexural Modulus 0.379 GPa
55.0 ksi
ASTM D790
Teknor Apex Telcar® TL-1000-105UV Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Flexural Modulus 0.379 GPa
55.0 ksi
ASTM D790
Teknor Apex Telcar® TL-94-T1422A-100 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec..
Flexural Modulus 0.379 GPa
55.0 ksi
ASTM D790
Lubrizol Estane® ALR CL65D Thermoplastic Polyurethane
Type: Estane® ALR CL650 is an aliphatic, polycaprolactone-based TPU with a Shore D Durometer of 65.Features: Contains a UV package that enhances outdoor weatherability. This high performance resin..
Flexural Modulus 0.379 - 0.7198 GPa
55.0 - 104.4 ksi
ASTM D790
Buckeye Polymers BP FLEX D0850 BLK Thermoplastic Polyolefin
Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist..
Flexural Modulus 0.379 GPa
55.0 ksi
Injection molded specimen, 0.05 in/min, Tangent method; ASTM D790
Phillips Sumika Marlex® CHP-055 Thermoplastic Polyolefin  (discontinued **)