Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.10 GPa | 885 ksi | Tangent; ASTM D790 |
RheTech Products F49-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Fan shroudsSupport ductsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | ISO 178 |
Radici Radilon® A RCV3015 RKC Nylon 66-GF30 Automotive cooling liquid resistant PA66-GF30 grade designed to be processed by GIT technology.Information provided by Radici group. |
|||
Flexural Modulus | 6.10 GPa @Temperature 23.0 °C |
885 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® HTN 52GM50EF WT001 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN52GM50EF WT001 is a glass and mineral reinforced high performance polyamide resin developed for LED reflector applications. It is also a PPA resin.Information provided by DuPont Performan.. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | 2mm/min; ASTM D790 |
Kingfa PA66-G15 15% Glass Fiber Reinforced PA66 Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t.. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | cond., 2 mm/min; ISO 178-A |
Lanxess Durethan® AM 40 X H2.0 901510 Nylon 66, Glass Fiber/Mineral Reinforced PA 66, 40% glass fibers/mineral, injection molding, heat-aging stabilized, low tendency to warpInformation provided by LANXESS. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP IFL34 PA 6/12 LNP* LUBRICOMP* IFL34 is a compound based on Nylon 6/12 resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP IFL34 PA 6/12 (Asia Pacific) LNP* Lubricomp* IFL34 is a compound based on Nylon 6/12 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY DX08333 PC (Asia Pacific) LNP Lubriloy* DX08333 is an internally lubricated compound based on Lexan* Polycarbonate resin. Added features of this material include: ESD Safe, PTFE-free Wear & Friction solution and balanced mec.. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DF004XXC PC (Europe-Africa-Middle East) Polycarbonate compound, countaining Glass Fiber |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON KEL22A Acetal Homopolymer (Europe-Africa-Middle East) LNP* LUBRICOMP* KEL22A is a compound based on Acetal Homopolymer resin containing Carbon Fiber, PTFE. Added features include: Electrically Conductive, Internally Lubricated. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 451E PBT (Europe-Africa-Middle East) VALOX 451E is 20% glass reinforced, flame retardant PBT injection moulding resin. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX.. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN133GL (COND, 50% RH) Nylon 66, 33% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN133GLUV (COND, 50% RH) Nylon 66, 33% Glass Fiber Reinforced, Internally Lubricated, UV Stabilized Information provided by Chase Plastics. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN230GL (COND, 50% RH) Nylon 66, 33% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | ASTM D790 |
Plenco 7202 Phenolic, Granular, Injection Molded PLENCO 07202 is an organic fiber reinforced phenolic molding compound, formulated to offer improved mechanical strength properties with an industrial finish. UL recognized under component file E4065.. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | ISO 178 |
Polyplastics Duranex® HN7315 Polybutylene Terephthalate (PBT), Low warpage, 15% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 6.10 GPa @Temperature 160 °C |
885 ksi @Temperature 320 °F |
ISO 178 |
DSM Stanyl® OCD2300 BLK PA46-GF50 50% Glass Reinforced, Heat Stabilized |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6600 GV 20 HWCP 20% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® HTN 52GM50EF WT001 Polyphthalamide (PPA)
(Unverified Data**) 50% Glass/Mineral Reinforced PPA High Performance Polyamide Zytel HTN52GM50EF WT001 is a glass and mineral reinforced high performance polyamide resin developed for LED reflector applications. It is.. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | ISO 178 |
Eurostar Star X 1615 33V S4 PA66, Glass Fiber Reinforced, UV stabilized, Injection Molding Star X 1615 33V S4 is an Impact Modified, Glass Fiber Reinforced, UV stabilized Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Dry as Molded Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent .. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R228 Nylon 66, 40% Mineral Reinforced, DAM Vydyne® R228 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in black, it is an injection-molding grade formulated to retain the inherent processing advant.. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | 2 [mm/min]; ISO 178 |
Akro-Plastic Akromid® B3 GF 20 (2470) PA 6 Dry, 20% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | ISO 527 |
BASF Ultramid® B35G3 BK 00564 15% Glass Filled PA6 (Dry) Description: 15% glass fiber reinforced injection molding grade e.g. for internal gas pressure applications such as flashing direction switch gears, automobile mirror housings and wheels of mountain.. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | 2 mm/min; ISO 178 |
Covestro Makroblend® UT4045 G PC/PBT Blend, 20% Glass Filled Main characteristics:• High toughness even at low temperatures• Good chemical resistance• Good paintability• Good flowability• Low moisture intakeGrade characteristics:• Excellent chemic.. |
|||
Flexural Modulus | 6.10 GPa | 885 ksi | ISO 178-93 |
Wellman Wellamid® MRB40K004-WT1 40% Mineral Reinforced Nylon 66 Description: Mineral Reinforced Nylon 66Information provided by Wellman. |