Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 61.4 GPa @Temperature 21.1 °C |
8900 ksi @Temperature 70.0 °F |
Dry, 90° Direction; ASTM D790 |
Renegade Materials Corporation RM-3002 Bismaleimide (BMI) Resin T650-35-6K-UC309-5HS Carbon Fabric Developed using state-of-the-art formulating technologies, RM-3002 BMI prepreg products deliver superior hot/wet performance in airframe, missile and propulsion applications at service temperatures .. |
|||
Flexural Modulus | 61.4 GPa @Temperature 177 °C |
8900 ksi @Temperature 350 °F |
Dry, 90° Direction; ASTM D790 |
Renegade Materials Corporation RM-3002 Bismaleimide (BMI) Resin T650-35-6K-UC309-5HS Carbon Fabric Developed using state-of-the-art formulating technologies, RM-3002 BMI prepreg products deliver superior hot/wet performance in airframe, missile and propulsion applications at service temperatures .. |