Mechanical Properties Metric English Comments
Flexural Modulus 4.45 GPa
645 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS (Asia Pacific)
PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 4.45 GPa
645 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS (Asia Pacific)
PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 4.45 GPa
645 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS (Europe-Africa-Middle East)
PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Modulus 4.45 GPa
645 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS (Europe-Africa-Middle East)
PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Modulus 4.45 GPa
645 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS
Reinforced PC/ABS with high stiffness and low CTE.
Flexural Modulus 4.45 GPa
645 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS
Reinforced PC/ABS with high stiffness and low CTE.
Flexural Modulus 4.45 GPa
645 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS (Asia Pacific)
Reinforced PC/ABS with high stiffness and low CTE.
Flexural Modulus 4.45 GPa
645 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS (Asia Pacific)
Reinforced PC/ABS with high stiffness and low CTE.
Flexural Modulus 4.45 GPa
645 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS (Europe-Africa-Middle East)
Reinforced PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Modulus 4.45 GPa
645 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS (Europe-Africa-Middle East)
Reinforced PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Modulus 4.45 GPa
645 ksi
ASTM D790
Polymer Resources TP-HG15 Polybutylene Terephthalate, 15% Glass Reinforced Alloy
Polybutylene Terephthalate, 15% Glass Reinforced AlloyProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informatio..
Flexural Modulus 4.45 GPa
645 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP SF004S PA12
LNP* Thermocomp* SF004S is a compound based on Nylon 12 containing 20% glass fiber. Added features include: Heat Stabilized, Healthcare
Flexural Modulus 4.45 GPa
645 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp ZZ006 PPE+PS (Asia Pacific)
LNP* THERMOCOMP* ZZ006 is a compound based on PPE+PS Blend resin containing Milled Glass.This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 4.45 GPa
645 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS
PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 4.45 GPa
645 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS
PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Americas region.