Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.65 GPa | 1110 ksi | ASTM D790 |
Owens Corning Glass Fiber Reinforced Nylon 6, 30 wt.% glass Nylons, as a group, are inert to most organic solvents. They resist alkalis and salt solutions and they are attacked by strong mineral acids and oxidizing agents. Data provided by the manufacturer,.. |
|||
Flexural Modulus | 7.65 GPa @Thickness 3.20 mm |
1110 ksi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical LUMID EG2309B(W) PA66+GF30%, Chemical Resistance(CaCl2, Ethylene Glycol) Feature: Injection Molding, PA66+GF30%, Chemical Resistance(CaCl2, Ethylene Glycol)Application: Radiator Tank, Intercooler TankCAS No. 32131-17-2, 65997-17-3 and 9010-79-9Information provided by LG .. |
|||
Flexural Modulus | 7.65 GPa @Thickness 3.20 mm |
1110 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMID GN-2251BF Flame Retardant PA Alloy Feature: Injection Molding, Flame Retardant PA AlloyApplication: E&E partsInformation provided by LG Chemical |
|||
Flexural Modulus | 7.65 GPa @Thickness 3.20 mm |
1110 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® GP2300G PBT+GF30% Description: Injection Molding, PBT+GF30%, HCFC ResistanceApplication: E&E (Muffler of Refrigerator)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Flexural Modulus | 7.65 GPa | 1110 ksi | ASTM D570 |
LG Chemical Lupox® PBT-GP-2300 30% GFR PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 7.65 GPa | 1110 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DE0029EF PC LNP STAT-KON* DE0029EF is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding. Flame Retardant, Electrically Conductive. |
|||
Flexural Modulus | 7.65 GPa | 1110 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DEP42E PC LNP STAT-KON* DEP42E is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 20% PTFE/Silicone. Added features of this material include: Easy Molding. Electrically Conductive, Wear.. |
|||
Flexural Modulus | 7.65 GPa | 1110 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DEP42E PC (Asia Pacific) LNP STAT-KON* DEP42E is a compound based on Polycarbonate resin containing Silicone, PTFE, Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 7.65 GPa | 1110 ksi | |
Shinil Chemical SHINFLAME PA-6 GF Flame Retardant Polymer Parts SHINFLAME is a flame retardant (FR) compound which exhibits inherent flame retardant properties during fire. Shinil uses its patented dispersion blending technology with variety of polymers to prod.. |
|||
Flexural Modulus | 7.65 GPa | 1110 ksi | ASTM D790 |
Samyang Trirex® SF3200GNH20 Polycarbonate, Reinforced Non Halogen for Printers PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.SF3200GNH20 is a reinforced, non-halogen grade for Printers.Applications: Office Machi.. |
|||
Flexural Modulus | 7.65 GPa | 1110 ksi | ASTM D790 |
PlastxWorld CEVIAN® VGR30 30% GF ABS Glass fiber reinforced ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Flexural Modulus | 7.65 GPa | 1110 ksi | 2.8mm/min; ASTM D790 |
Asia International Enterprise (Hong Kong) 30G6 Polybutylene terephthalate, 30% Glass Fiber Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Flexural Modulus | 7.65 GPa | 1110 ksi | 5 mm/min; ISO 178 |
Gromax CFG30-SN31N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |