Polymer Property : Flexural Modulus = 76.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.524 GPa
76.0 ksi
Method I (3 point load), Procedure B); ASTM D790
Multibase Multi-Flex® D 5308 HF Black TPO Thermoplastic Polyolefin Elastomer
Forms: PelletsInformation provided by Multibase
Flexural Modulus 0.524 GPa
76.0 ksi
2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 B
Dow DNDA-1081 NT 7 Linear Low Density Polyethylene Resin
DOW DNDA-1081 NT 7 is produced using UNIPOL™ PE process technology. It is intended for high-speed injection molding of thin walled parts such as downguaged lids. Information provided by Dow
Flexural Modulus 0.524 GPa
76.0 ksi
2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 B
Dow DNDA-1149 NT 7 Linear Low Density Polyethylene Resin
DOW DNDA-1149 NT 7 is produced using UNIPOL™ PE process technology and is intended for high-speed injection molding applications. Information provided by Dow
Flexural Modulus 0.524 GPa
76.0 ksi
2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 B
Dow DNDA-9810 NT 7 Linear Low Density Polyethylene Resin
DOW DNDA-9810 NT 7 is produced using UNIPOL™ PE process technology and is supplied in pellet form. This resin is specifically designed as a carrier resin for color concentrates and other masterbat..
Flexural Modulus 0.524 GPa
76.0 ksi
2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 B
Dow DNDB-1077 NT 7 Linear Low Density Polyethylene Resin
DOW DNDB-1077 NT 7 is produced using UNIPOL™ PE process technology. It is intended for high-speed injection molding of thin walled parts such as downguaged lids. Information provided by Dow