Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.80 GPa | 1280 ksi | 1.3 mm/min; ASTM D790 |
Ovation Polymers Opnyl OP6GF50 Nylon 6, 50% Glass Reinforced, Conditioned Nylon 6 - Glass reinforced (50 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. For Nylon compounds the m.. |
|||
Flexural Modulus | 8.80 GPa @Temperature 23.0 °C |
1280 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANMID 6 B12^ F30 Nylon 6, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 8.80 GPa @Temperature 23.0 °C |
1280 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANMID 6 B12^ QF2010 Nylon 6, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 8.80 GPa @Temperature 23.0 °C |
1280 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANMID 6 B13^ F30 Nylon 6, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 8.80 GPa @Temperature 23.0 °C |
1280 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANMID 6 B22^ E F40 Nylon 6, Glass Fiber Reinforced, Modified Information provided by Polykemi AB |
|||
Flexural Modulus | 8.80 GPa | 1280 ksi | ISO Value |
BASF Capron® 5233G 33% Glass-Filled Nylon 66 (Dry)
(discontinued **) Capron 5233G is a 33% glass fiber reinforced, polyamide 6,6 injection molding compound offering excellent strength, stiffness, creep resistance and dimensional stability. This balance of engineerin.. |
|||
Flexural Modulus | 8.80 GPa | 1280 ksi | 2mm/min; ASTM D790 |
Kingfa PA66-RG301 Flame Retardant, 30% Glass Fiber Reinforced PA66 Features:Flame retardantHigh strengthHigh temperature propertiesGood electric propertiesNo bloomingApplications:Injection moldingConnectorsRelayBobbinsPlugsInformation Provided by Kingfa Sci. & Tech.. |
|||
Flexural Modulus | 8.80 GPa | 1280 ksi | 2mm/min; ASTM D790 |
Kingfa PBT-RG30 Flame Retardant, 30% Glass Fiber Reinforced PBT Features:Flame retardantHigh strengthHigh temperature propertiesOutstanding electrical propertiesGood heat resistanceApplications:Injection moldingConnectorsRelayBobbins, plugsE & E partsInformation.. |
|||
Flexural Modulus | 8.80 GPa | 1280 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP EFL36E PEI (Europe-Africa-Middle East) LNP* Lubricomp* EFL36E is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 8.80 GPa | 1280 ksi | ISO 178 |
Solvay TECHNYL® R CR 218 V30 Nylon 6, 30% glass fiber, DRY TECHNYL® CR 218 V30 is a polyamide 6, reinforced with 30% glass fiber, heat stabilized, for injection molding. It contains recycled raw materials. This product is available in black color.Benefit.. |
|||
Flexural Modulus | 8.80 GPa | 1280 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36SXS PA 66 (Europe-Africa-Middle East) LNP* LUBRICOMP* RFL36SXS is a compound based on PA 66 resin containing Glass Fiber, PTFE. Added features include Internally Lubricated, Heat Stabilized. |
|||
Flexural Modulus | 8.80 GPa | 1280 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DE0029EF PC LNP STAT-KON* DE0029EF is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding. Flame Retardant, Electrically Conductive. |
|||
Flexural Modulus | 8.80 GPa | 1280 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp DF0069E PC LNP* Thermocomp* DF0069E is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.This data was supplied by SABIC.. |
|||
Flexural Modulus | 8.80 GPa | 1280 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp DF0069E PC (Asia Pacific) LNP* Thermocomp* DF0069E is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.This data was supplied by SABIC.. |
|||
Flexural Modulus | 8.80 GPa | 1280 ksi | ISO 178 |
Solvay TECHNYL® A 216 V33 PA66, 33% glass fiber, DRY Description: TECHNYL® A 216 V33 is a polyamide 66, reinforced with 33% of glass fiber, for injection molding. This product is available in natural color.Benefits: The product offers an excellent .. |
|||
Flexural Modulus | 8.80 GPa | 1280 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® 830 PBT (Europe-Africa-Middle East) VALOX 830 is a 30% glass fibre reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
Flexural Modulus | 8.80 GPa | 1280 ksi | ASTM D790 |
Plenco 3356 Phenolic, Granular, Injection Molded PLENCO 03356 is a mineral filled phenolic molding compound offering excellent arc resistance, comparative tracking, and flame resistant properties. UL recognized under component file E40654. 03356 i.. |
|||
Flexural Modulus | 8.80 GPa | 1280 ksi | ASTM D790 |
Plenco 4466 Phenolic, Granular, Injection Molded PLENCO 04466 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength and cosmetic properties. UL recognized under component file E40654. 04466.. |
|||
Flexural Modulus | 8.80 GPa | 1280 ksi | ASTM D790 |
Plenco 7500 Phenolic, Granular, Compression Molded PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi.. |
|||
Flexural Modulus | 8.80 GPa | 1280 ksi | ISO 178-93 |
Wellman Wellamid® GF30-60 42LH-NBK1 30% Glass Fiber Reinforced Nylon 6 Description: Glass Fiber Reinforced Nylon 6Information provided by Wellman. |
|||
Flexural Modulus | 8.80 GPa | 1280 ksi | ISO 178 |
Polyram RamSter PF310G6 PBT Alloy, 30% Glass Fiber, UV Stabilized 30% Glass fiber reinforced PBT alloy, low warp properties, UV stabilized for injection molding.Information provided by Polyram. |
|||
Flexural Modulus | 8.80 GPa | 1280 ksi | ASTM D790 |
Toyobo VYLOPET® EMC310TU Injection Molding Polyester Resin, Warpageless, High cycles Applications: Coiled bobbinsMouthpiecesFeatures: High cyclesWarpagelessInformation provided by Toyobo. |
|||
Flexural Modulus | 8.80 GPa | 1280 ksi | ASTM D790 |
Plenco 4301 Phenolic, Granular, Compression Molded PLENCO 04301 is a heat resistant, mineral filled phenolic molding compound offering excellent dimensional stability and electrical properties. UL recognized under component file E40654. 04301 is ava.. |
|||
Flexural Modulus | 8.80 GPa | 1280 ksi | cond; ISO 178 |
DSM Novamid® 1013G45 1 NA PA6-GF45 45% Glass Reinforced, Injection Molding |
|||
Flexural Modulus | 8.80 GPa | 1280 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6000 GV 35 HWCP 35% Glass Fiber Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 8.80 GPa | 1280 ksi | ISO 178 |
Eurostar Star L PA66 30V D51 PA66, Glass Fiber Filled, Injection Molded Star L PA66 30V D51 is a PTFE lubricated, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 8.80 GPa | 1280 ksi | ASTM D790 |
Adell AW-17 Nylon 66, 35% Glass Reinforced; Superior Finish Data provided by Adell Plastics, Inc. |
|||
Flexural Modulus | 8.80 GPa | 1280 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R633 Nylon 66 Copolymer, 33% Glass Filled, Dry as Molded Vydyne® R633 is 33% glass-fiber reinforced, PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold .. |
|||
Flexural Modulus | 8.80 GPa @Temperature 23.0 °C |
1280 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® 73G30TGI BK267 Nylon 6
(Unverified Data**) Zytel® 73G30TGI BK267 is a 30% glass fiber reinforced, toughened, black polyamide 6 optimized for gas injection molding process.Information provided by DuPont Performance Polymers |