Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.70 GPa | 827 ksi | STN EN ISO 178 |
Plastcom SLOVALEN PC 69 GF 35 FRT 4 Polypropylene Copolymer, 35% Glass Fiber, Halogen Free and Phosphor Free Flame Retardant FeaturesModified copolymer PP for injection moulding, chemically reinforced with 35% glass fiber, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. I.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | |
Plastcom SLOVAMID 66 GF 10 FRA 3 PA66, 10% glass fibre Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | STN EN ISO 178 |
Plastcom SLOVAMID 66 GF 25 FRG 5 Polyamide 66, 25% Glass Fiber, Halogen Free Flame Retardant FeaturesPA 66 for injection moulding, chemical reinforced with 25% glass fiber and non-halogen flame retardant, with heat and flammability resistance, achieves V-0 in accordance with UL 94. Non-hal.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | |
Plastcom SLOVAMID 66 GF 25 FRI 3 TS PA66, 25% glass fibre, flame retardant FeaturesPA 66 for injection moulding, chemically reinforced with 25% glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 in accordance with UL 94. Non.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ISO 178, ASTM D790 |
Nilit Nilamid A3 H G3 15% Glass Reinforced PA66 Description: Nilamid A3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 66. This product combines good overall mechanical performance and impact strength with ease of processing.Key char.. |
|||
Flexural Modulus | 5.70 GPa @Temperature 60.0 °C |
827 ksi @Temperature 140 °F |
ASTM D790 |
LATI LATAN 13 G/303 30% Glass Fiber Reinforced Polyoxymethylene Copolymer (POM)
(discontinued **) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 15 H2.0 DUS008 901510 Nylon 6, Glass Fiber Reinforced PA 6, 15% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 20 FN20 000000 Nylon 6, Glass Fiber Reinforced, Flame Retardant PA 6, 20% glass fibers, injection molding, halogen-free flame retardantInformation provided by LANXESS. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl PX7446 PPE+PS This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP WFL33 PBT LNP* LUBRICOMP* WFL33 is a compound based on PBT containing 15% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY AF306 ABS (Asia Pacific) LNP* Stat-loy* AF306 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. Added features of this material include: Antistat. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DF004 PC (Europe-Africa-Middle East) LNP* THERMOCOMP* DF004 is a compound based on Polycarbonate resin containing Glass Fiber. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ASTM D790 |
Techmer ES Plaslube® J-1/20/MS/5 NAT PA66 |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ASTM-D790 |
Polyram RamLloy PA917G4 PP/NYLON 66 alloy, 20% Glass Fiber 20% glass fiber reinforced PA66/PP alloy with reduced water absorption, dimensional stability and UV stabilized for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ASTM-D790 |
Polyram RamOfin PPH300G6 Polypropylene, 30% Glass Fiber 30% glass fiber reinforced polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | cond; ISO 178 |
DSM Novamid® 1017GH33 BK701 PA6-GF33 33% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ISO 178 |
DuPont Performance Polymers Sorona® 3015GV BK001 Polytrimethylene Terephthalate (PTT) 15% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3015GV BK001 is a 15% glass reinforced black PTT resin containing 31% renewably sourced ingredients by weight (37% based .. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | 50%RH; ISO 178 |
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6
(Unverified Data**) 30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T BK261 is a 30% glass fiber reinforced toughened black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polym.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ISO 178 |
Eurostar Starflam PX05003 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PX05003 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ISO 178 |
Azdel Plus R401B02N 40% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R401B02N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | cond.; ISO 178 |
Azoty Tarnow™ Tarnamid® T-27 GF30 I Polyamide 6 - Glass Fiber Reinforced 30% Glass fiber reinforced, impact modified, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following mai.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R525H BK02 Nylon 66, 25% Glass Reinforced, Conditioned Vydyne® R525H BK02 is high-flow, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R525H BLK Nylon 66, 25% Glass Reinforced, Conditioned Vydyne® R525H BLK is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ASTM D790 |
A. Schulman ComAlloy Aqualoy® 145 Polypropylene, Glass Reinforced, Chemically Coupled NSF Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced. In Aqualoy® materials, carefully selected base resins and proprietary additives meld hydrolytic stability an.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 413 Glass Reinforced, Polycarbonate/Polyester Alloy, UL Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | 50%RH; ISO 178 |
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6
(Unverified Data**) 30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T NC010 is a 30% glass fiber reinforced toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 5.70 GPa @Temperature 120 °C |
827 ksi @Temperature 248 °F |
ASTM D790 |
LATI LASULF G/20 20% Glass Reinforced Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Flexural Modulus | 5.70 GPa | 827 ksi | ASTM D790 |
PolyOne Lubri-Tech™ ES-20GF/15T Polyethersulfone - 20% Glass Fiber Reinforced - 15% PTFE Lubricated
(disconti Data provided by PolyOne. |
|||
Flexural Modulus | 5.70 GPa @Temperature 23.0 °C |
827 ksi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Sorona® 3015G BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& Sorona® 3015G BK001 is a 15% glass reinforced black PTT resin containing 31% renewably sourced ingredients by weight (37% polymer basis) with good strength, stiffness and low warpage and superior s.. |