Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.90 GPa | 856 ksi | |
Plastcom SLOVAMID 66 T 36 TS PA66, 36% mineral filling FeaturesPA 66 with the content of 36 % chemically modified mineral filling. Used for holders of electric hand tools, for hobby tools, gears, covers of electric tools, flat products, automobile wheel.. |
|||
Flexural Modulus | 5.90 GPa @Temperature 23.0 °C |
856 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYblend 85FS GF20 PC/ABS-Blend, Glass Fiber reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 5.90 GPa @Temperature 23.0 °C |
856 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPH GF5020 HC Polypropylene Homopolymer, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | ASTM D790 |
LG Chemical LUCEL MR-320 Low Warpage POM, 20% Mineral Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | cond., 2 mm/min; ISO 178-A |
Lanxess Durethan® AKV 30 000000 Nylon 66, Glass Fiber Reinforced PA 66, 30% glass fibers, injection moldingInformation provided by LANXESS. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP KFL23LH Acetal Copolymer LNP LUBRICOMP* KFL23LH is a compound based on Acetal Copolymer resin containing 15% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Low Extractable. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | 2 mm/min, 64mm span; ISO 178 |
SABIC Innovative Plastics SABIC STAMAX 30YM240 PP SABIC® STAMAX 30YM240 is a 30% long glass fiber reinforced polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMDS is 16496906... |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | 2 mm/min, 64mm span; ISO 178 |
SABIC Innovative Plastics SABIC STAMAX 30YM243 PP SABIC® STAMAX 30YM243 is a 30% long glass fiber reinforced UV stabilized polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMD.. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP SFL36 PA12 (Europe-Africa-Middle East) LNP* LUBRICOMP* SFL36 is a compound based on PA 12 resin containing Glass Fiber, PTFE. Added features include: Internally Lubricated. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® 412 PBT (Europe-Africa-Middle East) VALOX 412 is 20% glass reinforced PBT injection moulding resin. Applications: Spotlights, appliance housings and handles. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON PFD04 PA 6 LNP* STAT-KON* PFD04 is a compound based on Nylon 6 containing 20% Glass Fiber. Added feature of this grade is: Ellectrically Conductive. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP JF004 PES (Europe-Africa-Middle East) LNP* Thermocomp* JF004 is a compound based on Polyethersulfone resin containing Glass Fiber. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF0029S PA 66 LNP* THERMOCOMP* RF0029S is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | ISO 178 |
Solvay TECHNYL® A 218HP V30 Black 21N PA66, 30% glass fiber, Conditioned Provisional datasheet - Product in developmentDescription: Polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYLÂ.. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Asia Pacific) Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | ISO 178 |
Solvay Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH50 Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Technyl A 216 V30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical prope.. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | ISO 178 |
Polyram RamOfin PPH308G6 Polypropylene, 30% Glass Fiber, Impact Modified 30% Glass fiber reinforced, heat stabilized, impact modified polypropylene for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | DAM; ISO 178 |
DuPont Performance Polymers Minlon® 73M40 NC010 Nylon 6
(Unverified Data**) 40% Mineral Reinforced Polyamide 6 Minlon 73M40 NC010 is a 40% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro.. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | ASTM D790 |
Adell ER-36 Homopolymer Polypropylene, 30% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 113 Polypropylene, Glass Reinforced, Chemically Coupled Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | Dry; ASTM D790 |
Asahi Kasei Leona® CR301 Nylon 66 Suitable for a switch insulator. Low abrasion and superior electrical properties.Applications:Sliding switch insulators Information provided by Asahi Kasei |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | At 2 mm/min; ISO 178 |
Borealis Xmod™ K65G3 30% Glass Fiber Reinforced Polypropylene Compound Xmod K65G3 is a 30% glass fiber reinforced grade intended for injection molding. Xmod K65G3 has been developed especially for the car industry, to be used UTB parts. Xmod K65G3 offers good balance.. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | ASTM D790 |
LATI LASULF G/20 20% Glass Reinforced Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | ASTM D790 |
Adell BJ-17 Nylon 6, 35% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Flexural Modulus | 5.90 GPa | 856 ksi | ASTM D790 |
Adell ER-16 Homopolymer Polypropylene, 30% Glass Reinforced Data provided by Adell Plastics, Inc. |