Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 9.10 GPa | 1320 ksi | ASTM D790 |
LATI LAESTRA G/30 30% Glass Fiber Reinforced Syndiotactic Polystyrene (SPS)
(discontinued **) Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270.. |
|||
Flexural Modulus | 9.10 - 12.0 GPa | 1320 - 1740 ksi | Average value: 10.2 GPa Grade Count:6 |
Overview of materials for Liquid Crystal Polymer (LCP), Unfilled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Unfilled". Each property range of values reported is minimum and maximum v.. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 135 DUS008 000000 Nylon 6, 35% Glass Fiber PA 6, 35% glass fibers, injection molding, impact modifiedInformation provided by LANXESS. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ISO 178 |
Lanxess Pocan® B 3233 HR 000000 Polybutylene Terephthalate, 30% Glass Fibers PBT, 30% glass fibers, injection molding, improved flowability, hydrolysis stabilized |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP KFL25 Acetal Copolymer LNP LUBRICOMP* KFL25 is a compound based on Acetal Copolymer resin containing 25% Glass Fiber, 10% PTFE. Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DEP23FXC PC LNP STAT-KON* DEP23FXC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 10% PTFE/Silicone. Added features include: Electrically Conductive. Wear Resistant, Superior Molding. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® ENH4550 PBT 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® IQ420 PBT (Asia Pacific) Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® IQ420HP PBT (Asia Pacific) Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® V9260CS PET (Asia Pacific) Color Stable Glass filled PET |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP IX95700 PA6.12 LNP* THERMOCOMP* IX95700 is a compound based on Nylon 6/12 resin containing Glass Fiber. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp RF007ESS PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RF007ESS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.This data was supplied by SABIC-IP for.. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RF008ESY PA 66 LNP THERMOCOMP* RF008ESY is a compound based on Nylon 66 resin containing 40% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP WF006 PBT LNP THERMOCOMP* WF006 is a compound based on PBT resin containing 30% Glass Fiber. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DEP23FXC PC (Asia Pacific) LNP STAT-KON* DEP23FXC is a compound based on Polycarbonate resin containing Silicone, Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DX95523C PC LNP* STAT-KON* DX95523C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DX95523C PC (Asia Pacific) LNP* Stat-kon* DX95523C is a compound based on Polycarbonate resin. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® IQ420HP PBT Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® IQ420HP PBT Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® IQ420HP PBT (Europe-Africa-Middle East) Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ISO 178 |
Polyplastics Duranex® 330HR Polybutylene Terephthalate (PBT), Hydrolysis resistant, Heat shock resistant, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ASTM D790 |
Plenco 4002 Phenolic, Granular, Injection Molded PLENCO 04002 is a heat resistant, mineral filled phenolic molding compound offering excellent mechanical strength and dimensional stability at elevated temperatures. UL recognized under component fi.. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ISO 178 |
Polyplastics Duranex® 3306 Polybutylene Terephthalate (PBT), Higher gloss, Better surface appearance, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | 2 mm/min; ISO 178 |
Eurostar Staramide RF007ESS PA66/6, 35% Glass Filled, Injection Molded Staramide RF007ESS is a 35% Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as RF1007EMHS)Information provided by Eurostar. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 243 SAN, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DX07408 PC LNP* THERMOCOMP* DX07408 is a compound based on Polycarbonate containing Proprietary Filler(s). Added feature of this grade is: UL Rated. |