Polymer Property : Flexural Modulus = 9.34 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 9.34 GPa
1350 ksi
ASTM D790
SABIC Innovative Plastics LNP VERTON MV00AS PP (Asia Pacific)
LNP VERTON* MV00AS is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
Flexural Modulus 9.34 GPa
1350 ksi
ASTM D 790
SABIC Innovative Plastics LNP Verton MX03017 PP (Europe-Africa-Middle East)
LNP* VERTON* MX03017 is a compound based on Polypropylene resin containing Glass Fiber, Long Glass Fiber. Added features of this material include: Chemically Coupled.This data was supplied by SABIC..
Flexural Modulus 9.34 GPa
1350 ksi
ASTM D790
SABIC Innovative Plastics LNP VERTON MV00ASXP PP (Europe-Africa-Middle East)
LNP VERTON* MV00AS is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
Flexural Modulus 9.34 GPa
1350 ksi
ASTM D790
SABIC Innovative Plastics LNP VERTON MV00AS PP
LNP VERTON* MV00AS is a compound based on Polypropylene resin containing 50% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, Structural.
Flexural Modulus 9.34 GPa
1350 ksi
ASTM D790
SABIC Innovative Plastics LNP VERTON MV00ASU PP
LNP VERTON* MV00ASU is a compound based on Polypropylene resin containing 50% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, UV Stabilized, Structur..
Flexural Modulus 9.34 GPa
1350 ksi
ASTM D790
SABIC Innovative Plastics LNP VERTON MV00ASU PP (Asia Pacific)
LNP VERTON* MV00ASU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
Flexural Modulus 9.34 GPa
1350 ksi
ASTM D790
SABIC Innovative Plastics LNP VERTON MV00ASU PP (Europe-Africa-Middle East)
LNP VERTON* MV00ASU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.