Mechanical Properties Metric English Comments
Flexural Modulus 6.76 GPa
980 ksi
Tangent; ASTM D790
RheTech Products F55-01 43% Glass Fiber/Talc Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Consumer goodsSupportsGolf cart bracketsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 6.76 GPa
980 ksi
Tangent; ASTM D790
RheTech Products G40P100-00 40% Glass Fiber Reinforced Polypropylene, Natural
Injection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 6.76 GPa
980 ksi
Tangent; ASTM D790
RheTech Products G40P100-01 40% Glass Fiber Reinforced Polypropylene, Black
Injection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 6.76 GPa
980 ksi
Tangent; ASTM D790
RheTech Products GC40P101-00 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: Consumer goodsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 6.76 GPa
980 ksi
ASTM D790
PolyOne Nymax™ MF 1200 A 40 HS Natural Polyamide 66 (Nylon 66)
The Nymax® MF 1200 Series of mineral-reinforced nylon 6/6 compounds have been specifically engineered to provide an excellent balance of physical property performance, toughness, chemical resistanc..
Flexural Modulus 6.76 GPa
980 ksi
ASTM D790
Niche Polymer PPHG40BK Homopolymer PP, 40% Glass Fiber Filled
Information provided by Niche Polymer
Flexural Modulus 6.76 GPa
980 ksi
ASTM D790
Quadrant EPP Duratron® PAI T5030 Polyamide-imide, glass reinforced, extruded (ASTM Product Data Sheet)
Flexural Modulus 6.76 GPa
980 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRILOY DX08333 PC (Asia Pacific)
LNP Lubriloy* DX08333 is an internally lubricated compound based on Lexan* Polycarbonate resin. Added features of this material include: ESD Safe, PTFE-free Wear & Friction solution and balanced mec..
Flexural Modulus 6.76 GPa
980 ksi
ASTM D790
Techmer ES Electrafil® J-50/CF/10/TF/13/SI/2 Polycarbonate, 10% Carbon Fiber Reinforced, 13% PTFE, 2% Silicone
Flexural Modulus 6.76 GPa
980 ksi
ASTM D790
Techmer ES Electrafil® J-50/CF/10/TF/15 Polycarbonate, 10% Carbon Fiber Reinforced, 15% PTFE
Flexural Modulus 6.76 GPa
980 ksi
Tangent; ASTM D790
Plastics Group Polifil® GFPPCC-40 40% Glass Reinforced Polypropylene
Polifil® GFPPCC series compounds are homopolymer polypropylenes reinforced with chemically coupled glass fibers. These compounds offer superior strength and stiffness, improved elevated temperature..
Flexural Modulus 6.76 GPa
980 ksi
8 lb Core, 6 hrs @ 220°F, Vacuum Bag
Zyvex Performance Materials Aroply™ 250 Nano-Engineered Composite Film Adhesive
Aroply™ 250 Film Adhesive is a versatile, heat curing carbon-nanotube modified epoxy structural film adhesive available in a variety of film weights on a supported knitted nylon carrier. Cured adhe..
Flexural Modulus 6.76 GPa
980 ksi
BCC Products BC 6004 Epoxy Surface Coat
BC 6004 is a white thixotropic epoxy surface coat that has the ability to cure and bond to freshly poured wet plaster. This formulated resin compound can be applied with a brush or troweled to a thi..
Flexural Modulus 6.76 GPa
980 ksi
BCC Products BC 7009-1 Epoxy Casting
BC 7009-1 is an iron filled, low-cost mass casting system. Thicknesses up to two inches in non-conductive molds, and four inches in conductive molds can be achieved without foaming or yielding exces..
Flexural Modulus 6.76 GPa
980 ksi
ASTM D790
PolyOne Edgetek® ATH-25GF/000 Acetal-Homopolymer, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation.