Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Unnotched = 130 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Unnotched 176 J
130 ft-lb
PSM Industries PolyAlloys MIM-2700 sintered Low Alloy Steel
PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl..
Charpy Impact, Unnotched 176 J
130 ft-lb
1/2 size bar
Kinetics MIM F75 (ASTM F75) HIP
Most commonly used within the medical market on applications requiring these characteristics: Bio-compatibility Corrosion resistance High strength Nonmagnetic Wear resistance. Information prov..
Copyright © lookpolymers.com All Rights Reserved