Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 4.63 J | 3.42 ft-lb | Dow Method |
Dow TUFLIN™ HS-7065 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Good Processability at Narrow Die Gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7065 NT 7 is a fractional melt, ethylene-hexene copolymer, designe.. |
|||
Puncture Energy | 4.64 J | 3.42 ft-lb | Exxon Mobil Method |
ExxonMobil Exceed™ 3512CB Film Resin Exceed 3512CB resin is a hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3512CB resin have outstanding cold temperature toughness, impact strength and punc.. |
|||
Puncture Energy | 4.63 J | 3.42 ft-lb | Dow Method |
Dow TUFLIN™ HS-7046 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Slot Cast Extrusion Outstanding Drawdown Capability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HS-7046 NT 7 is an ethylene-hexene copolymer, designed f.. |