Puncture Energy 7.00 J

@Temperature -30.0 °C
5.16 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® BKV 130 000000 Copolyamide, 30% Glass Fiber
CoPA, injection molding grade, 30% glass fibers, elastomer modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 30, even in..
Puncture Energy 7.00 J

@Temperature -30.0 °C
5.16 ft-lb

@Temperature -22.0 °F
Conditioned; ISO 6603-2
Lanxess Durethan® BKV 130 000000 Copolyamide, 30% Glass Fiber
CoPA, injection molding grade, 30% glass fibers, elastomer modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 30, even in..
Puncture Energy 7.00 J

@Temperature -30.0 °C
5.16 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® BKV 130 H3.0 101006 Copolyamide, 30% Glass Fiber
CoPA, injection molding grade, 30% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 30 H3.0, ev..
Puncture Energy 7.00 J

@Temperature -30.0 °C
5.16 ft-lb

@Temperature -22.0 °F
Conditioned; ISO 6603-2
Lanxess Durethan® BKV 130 H3.0 101006 Copolyamide, 30% Glass Fiber
CoPA, injection molding grade, 30% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 30 H3.0, ev..
Puncture Energy 7.00 J
5.16 ft-lb
ISO 6603-2
Lanxess Durethan® BKV 230 H2.0 901510 Copolyamide, 30% Glass Fiber
CoPA, injection molding grade, 30% glass fibers, elastomer-modified, higher impact and notched impact strength and also higher energy absorption under biaxial impact load than BKV 130, conditioning ..
Puncture Energy 7.00 J

@Temperature -30.0 °C
5.16 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® BKV 35 HTS 901510 Nylon 6, 35% Glass Fiber
PA 6, injection molding grade, 35% glass fibers, very good heat-ageing resistance
Puncture Energy 7.00 J

@Temperature -30.0 °C
5.16 ft-lb

@Temperature -22.0 °F
Conditioned; ISO 6603-2
Lanxess Durethan® BKV 35 HTS 901510 Nylon 6, 35% Glass Fiber
PA 6, injection molding grade, 35% glass fibers, very good heat-ageing resistance
Puncture Energy 7.00 J
5.16 ft-lb
ISO 6603-2
Lanxess Durethan® BKV 30 HTS 901510 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, very good heat-ageing resistance
Puncture Energy 7.00 J
5.16 ft-lb
170N; ASTM D5748
Borealis FT3200 Low Density Polyethylene
FT3200 is a Low Density Polyethylene for Film Extrusion. Applications heavy-duty bags, shrink film, construction films, and agricultural films. FT3200 contains no additives.Information provided by..