Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 206 kN/m | 1180 pli | Die C; ASTM D624 |
SK Chemicals SKYTHANE® 155D S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tear Strength | 206 kN/m | 1180 pli | Die C; ASTM D624 |
SK Chemicals SKYTHANE® S155D Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tear Strength | 207 kN/m | 1180 pli | 2 in/min; ASTM D624 |
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass) Information provided by A. Schulman. |
|||
Tear Strength | 207 kN/m | 1180 pli | 2 in/min; ASTM D624 |
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass) Information provided by A. Schulman. |
|||
Tear Strength | 207 kN/m | 1180 pli | 2 in/min; ASTM D624 |
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass) Information provided by A. Schulman. |
|||
Tear Strength | 207 kN/m | 1180 pli | 2 in/min; ASTM D624 |
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass) Information provided by A. Schulman. |
|||
Tear Strength | 206 kN/m | 1180 pli | ASTM D624 |
Toyobo Pelprene™ P-280B Polyester TPE Key Feature: Pelprene P typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'P' type is a block.. |
|||
Tear Strength | 207 kN/m | 1180 pli | 2 in/min; ASTM D624 |
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass) Information provided by A. Schulman. |
|||
Tear Strength | 207 kN/m | 1180 pli | 2 in/min; ASTM D624 |
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass) Information provided by A. Schulman. |