Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tear Strength = 150 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 150 kN/m
856 pli
ASTM D624
GRECO ISOTHANE 1198A Poly(adipate)ester TPU Resin
ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp..
Tear Strength 150 kN/m
855 pli
Unnicked; ISO 34-1B
Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer
Type: Pearlthane® 11H98 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Extrusion/MouldingSpecial Features : Combining a unique set of properties such as mec..
Tear Strength 150 kN/m
856 pli
DIN 53515
Lubrizol ESTANE® ETE60DS3 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tear Strength 150 kN/m
856 pli
ASTM D624
Wanhua Chemical Wanthane® WHT-1495RV Polyester Based TPU
Good extrusion stability, high transparency, excellent mechanical propertiesInformation provided by Wanhua Chemical Group Co., Ltd.
Tear Strength 150 kN/m
856 pli
DIN 53515
Lubrizol ESTANE® 5799 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tear Strength 150 kN/m
856 pli
ISO 34
Chengdu Polyster CH7563 Thermoplastic Polyether-ester Elastomer (TPEE)
Poly-basic block copolymer. Good compatibility with PBT, PET and PA. For blending with PBT, PET and PA to improve impact resilience properties.Information provided by Chengdu Polyster Co., Ltd.
Tear Strength 150 kN/m
856 pli
ISO 34
Chengdu Polyster H6055 Thermoplastic Polyether-ester Elastomer (TPEE)
Medium modulus molding and injection grade. Contains improved color- stable antioxidants. Higher melt flow index compared with other grades; good balance of modulus and toughness. Applications requi..
Tear Strength 150 kN/m
856 pli
normal; ISO 34-1
DuPont Performance Polymers Hytrel® HTR8730 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Viscosity Polyester Elastomer with Excellent Mechanical Properties at Elevated Temperatures Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Tear Strength 150 kN/m
856 pli
notched; ASTM D624 (C)
Arkema Group Pebax® 6333 Polyether Block Amide (PEBA)
Information provided by Arkema Group
Tear Strength 150 kN/m
856 pli
ASTM D624
C.O.I.M. LARIPUR® LPR5450 Modified Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
Tear Strength 150 kN/m
856 pli
DIN ISO 34-1/Bb
BASF Elastollan 1154 D KFFC TPUR
Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien..
Tear Strength 150 kN/m
856 pli
DIN ISO 34-1/Bb
BASF Elastollan B 60 D TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup..
Tear Strength 150 kN/m
856 pli
ASTM D624
BASF Elastollan® S95A Polyester Type Polyurethane Elastomer
Recommended for injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fuel and solv..
Tear Strength 150 kN/m
856 pli
AorTech Biomaterials ECSil™ 60D Biomedical Carbonate Silicone Pellets
Elast-Eon™ Carbonate Silicone (ECSil™) is a family of next generation biomedical polymers. ECSil™ is finding strong interest in cardiac pacing leads, orthopaedics, spinal discs, and generally an..
Tear Strength >= 150 kN/m
>= 856 pli
ISO 34
Austin Novel Materials Texalan® 464D Polyester-based TPU
Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Tear Strength 150 kN/m
856 pli
DIN ISO 34-1/Bb
BASF Elastollan 598 A TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and a high abrasion resistance.Typical Applications: Heel top-pieces, castor tyres and parts requiri..
Tear Strength 150 kN/m
856 pli
DIN ISO 34-1/Bb
BASF Elastollan S 98 A TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat..
Tear Strength 150 kN/m
856 pli
AorTech Biomaterials ECSil™ 60D Biomedical Carbonate Silicone Pellets
Elast-Eon™ Carbonate Silicone (ECSil™) is a family of next generation biomedical polymers. ECSil™ is finding strong interest in cardiac pacing leads, orthopaedics, spinal discs, and generally an..
Copyright © lookpolymers.com All Rights Reserved