Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 18.0 kN/m | 103 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2610 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tear Strength | 18.0 kN/m | 103 pli | Die B |
Momentive Performance Materials TSE 221-6U Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 18.0 kN/m | 103 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 3286/70 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Tear Strength | 18.0 kN/m | 103 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 3486/35 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Tear Strength | 18.0 kN/m | 103 pli | |
Trelleborg E569 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Tear Strength | 18.0 kN/m | 103 pli | ASTM D624 |
ELASTO UK Dryflex® 500400S SEBS Based Material, Unfilled Qualities, 40A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tear Strength | 18.0 kN/m | 103 pli | ASTM D624 |
ELASTO UK Dryflex® 500450S SEBS Based Material, Unfilled Qualities, 45A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tear Strength | 18.0 kN/m | 103 pli | ASTM D624 |
ELASTO UK Dryflex® 600400S SEBS Based Material, Filled Qualities, 40A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tear Strength | 18.0 kN/m | 103 pli | ASTM D624 |
ELASTO UK Dryflex® 600450S SEBS Based Material, Filled Qualities, 45A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tear Strength | 18.0 kN/m | 103 pli | ISO 34-B |
AlphaGary Evoprene™ 027 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Tear Strength | 18.0 - 35.0 kN/m | 103 - 200 pli | ASTM D 624 |
API Megol AM SV/PS SEBS Adhesion Modified Overmolding for PS Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |
|||
Tear Strength | 18.0 kN/m | 103 pli | ISO 34-B |
AlphaGary Evoprene™ GC 5655 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |
|||
Tear Strength | 18.0 kN/m | 103 pli | Die B |
Momentive Performance Materials TUFEL™ III 92506 Biocompatible Extrusion Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |