Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 22.8 kN/m | 130 pli | ASTM D624 |
PolyOne Versaflex™ CL2050 Thermoplastic Elastomer (TPE) Versaflex™ CL2050 is an easy processing compound designed for use in applications where clarity and enhanced heat resistance are required. New Product. Commercial specifications have not been estab.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | ASTM D624 |
PolyOne Versaflex™ CL40 Thermoplastic Elastomer (TPE) Versaflex™ CL40 is an easy processing compound designed for use in injection molding applications where water-clarity and excellent colorability are required. - Excellent Clarity - Excellent Colora.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | ASTM D624 |
Network Polymers Softflex® 0350 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Tear Strength | 22.8 kN/m | 130 pli | ASTM D624 |
Multibase Multi-Flex® RP 6568 C Natural TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Tear Strength | 22.8 kN/m | 130 pli | Die B,molded-without post cure; ASTM D624 |
Multibase C6-235 DI-CUP R Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 22.8 kN/m | 130 pli | Die B,post cured- 2 hours at 177°C; ASTM D624 |
Multibase C6-235 DI-CUP R Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 22.8 kN/m | 130 pli | Die B, post cured- 4 hours at 177°C; ASTM D624 |
Multibase C6-235 DI-CUP R Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 22.8 kN/m | 130 pli | ASTM D624 |
Multibase Multi-Flex® A 6221 CUV Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Tear Strength | 22.8 kN/m | 130 pli | Initial Tear Strength |
Saint-Gobain CHR® 2925-7 Glass-Foil Backing Silicone Adhesive Pressure Sensitive Tape Description: For applications requiring higher tear strengths, fiberglass laminated with aluminum is available. Service temperatures range from -100°F to 500°F (-73°C to +260°C). This ta.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | Die C; ASTM D624 |
Teknor Apex Flexalloy® 9100-45 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | Die B |
Shin-Etsu Silicones KE-5530U Low Temperature Silicone Elastomer ShinEtsu KE5530 U is a nominal 30 Durometer phenyl (PVMQ) base.Product Features: This material was designed for its excellent vibration dampening characteristics. Because of its phenyl content, it a.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | ASTM D624 |
Teknor Apex Telcar® TL-1138 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | Trouser; ASTM D470 |
Lubrizol ESTANE® 58309 Ether Based Thermoplastic Polyurethane Features: Good Physical Properties and Reduced Surface Tack.Uses: Flat Die/Cast Film and Blown Film Extrusion, Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInfo.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | Trouser; ASTM D470 |
Lubrizol ESTANE® 58863 Ether Based Thermoplastic Polyurethane Features: Good Elasticity – High melt flow for easy processingUses: Extrusion – Wire and cable, general extrusionAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provi.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | |
Dow Corning HS II BASE & 10:1, COLORED CATALYST High strength silicone mold making rubber, suited for the detailed reproduction of fiines, art objects and similar items and better suited for thin section cure. HS II Base with HS II 10:1 Colored C.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | Die C; ASTM D 624 |
CPT C-Flex® R70-051 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | |
Dow Corning SILASTIC® P-1 RTV SILICONE RUBBER & CLEAR CURING AGENT High strength silicone rubber suited for prototyping, production tooling, artistic and renovation applications. Silastic P-1 is recommended for use with polyesters, cement and rigid polyurethanes; a.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | ASTM D624 |
Aearo E-A-R Specialty Composites VersaDamp™ V-2750 TPE VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® IT38-110 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerNaturalTranslucentApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:ExtrusionInjection MoldingPolyOne Fi.. |
|||
Tear Strength | 22.8 kN/m | 130 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® ST-6350 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Over-Molding GradeApplications:Multi-PurposeProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tear Strength | 22.8 kN/m | 130 pli | Trouser; ASTM D470 |
Lubrizol ESTANE® 58206 Ester Based Thermoplastic Polyurethane Features: Good Flexibility at Low Temperatures and Improved Weathering Performance.Uses: Flat Die/Cast Film Extrusion and Hose/Profile Extrusion, Injection Molding.Available in Americas, Europe, Mid.. |