Polymer Property : Tear Strength = 226 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 226 kN/m
1290 pli
Die C; ASTM D624
SK Chemicals SKYTHANE® 160D S series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tear Strength 226 kN/m
1290 pli
Die C; ASTM D624
SK Chemicals SKYTHANE® S160D Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Tear Strength 226 kN/m
1290 pli
Die C; ASTM D624
Lubrizol Estane® S160D Thermoplastic Polyurethane
Type: Estane® S160D is a Shore 63D, polyester based thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Americas, Europe, Middle East, ..
Tear Strength 226 kN/m
1290 pli
2 in/min; ASTM D624
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Tear Strength 226 kN/m
1290 pli
2 in/min; ASTM D624
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Tear Strength 226 kN/m
1290 pli
2 in/min; ASTM D624
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Tear Strength 226 kN/m
1290 pli
2 in/min; ASTM D624
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Tear Strength 226 kN/m
1290 pli
2 in/min; ASTM D624
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Tear Strength 226 kN/m
1290 pli
2 in/min; ASTM D624
A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.