Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 26.6 kN/m | 152 pli | Split; ASTM D624 |
Northstar Polymers MPP-A80H Room-Temperature Curable Polyurethane MPP-A80H has been specifically formulated to service applications where high elongation and good physical strength are required as well as where temperature during the process must be low for a very.. |
|||
Tear Strength | 26.6 kN/m | 152 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.0 PHR DBPH-50 MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 26.6 kN/m | 152 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Synprene® RT-3770 Styrene Butadiene Block Copolymer (SBC) with Mineral Filler
(discontinued **) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |
|||
Tear Strength | 26.6 kN/m | 152 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 4002 BLK Multi-Flex® A 4002 is based on Shell's Kraton G polymer and is suitable for soft touch applications for the automotive industry. It exhibits excellent paintibility adhesion. Multi-Flex TPE cont.. |
|||
Tear Strength | 26.6 kN/m | 152 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.0 PHR DBPH-50 MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 26.6 kN/m | 152 pli | |
Dow Corning SILASTIC® LS-2840 FLUOROSILICONE RUBBER 40 Durometer, off-white, uncatalysed, moulding grade fluorosilicone baseInformation provided by Dow Corning |
|||
Tear Strength | 26.6 kN/m | 152 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® IT 37-033 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledNaturalApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingDisclaimer: A therm.. |