Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 65.0 kN/m | 371 pli | Die C, 2 in/min; ASTM D1004 |
PolyOne Geon™ Vinyl Flexible 90067 Polyvinyl Chloride, Flexible (PVC, Flexible) Automotive OEM approval(s).Information provided by PolyOne |
|||
Tear Strength | 65.0 kN/m | 371 pli | Die C, 2 in/min; ASTM D1004 |
PolyOne Geon™ Vinyl Flexible 90071 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 65.1 kN/m | 371 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 310ºF Cure Temperature Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 65.0 kN/m | 371 pli | ISO 34-1 |
Huntsman IROGRAN® A 92 P 4851 Ether-Based TPU-For Cable Industry Introduction: IROGRAN A 92 P 4851 is a thermoplastic polyether- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are high extrudability and lo.. |
|||
Tear Strength | 65.0 kN/m | 371 pli | ISO 34B |
Huntsman AVALON® 70 AE Thermoplastic Polyurethane Introduction: AVALON 70 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 70 AE is part of the AVALON Soft Range and offers a premium soiling material .. |
|||
Tear Strength | 65.0 kN/m | 371 pli | Injection molded parts; ASTM D624 |
Huntsman IROGRAN® A 88 H 4622 TPU-Polyester Introduction: IROGRAN A 88 H 4622 is a black colored thermoplastic polyether/polyester-polyurethane for injection molding and extrusion applications. Additional characteristics of the product are hi.. |
|||
Tear Strength | 65.0 kN/m | 371 pli | ASTM D624 |
Sumitomo Chemical ESPOLEX® WT525 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Tear Strength | 65.0 kN/m | 371 pli | DIN 53515 |
Lubrizol ESTANE® T5213 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 65.0 kN/m | 371 pli | Die C; ASTM D1004 |
Teknor Apex TEKRON® 4300LM-P88-1 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tear Strength | 65.0 kN/m | 371 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.0 PHR Thanecure ZM Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man.. |
|||
Tear Strength | 65.1 kN/m | 371 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.75 PHR Zinc Stearate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 65.1 kN/m | 371 pli | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 65A Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 65.0 kN/m | 371 pli | Trouser Tear resistance MD; ISO 6383-1 |
EMS-Grivory Grivory® CF 6 S PA* Product description: Grilon CF 6 S is an extracted copolyamide with a low melting point. Very high flexibility and toughnessVery good thermoforming and orientation propertiesHigh shrinkVery good tra.. |
|||
Tear Strength | 65.0 kN/m | 371 pli | Trouser Tear resistance TD; ISO 6383-1 |
EMS-Grivory Grivory® CF 6 S PA* Product description: Grilon CF 6 S is an extracted copolyamide with a low melting point. Very high flexibility and toughnessVery good thermoforming and orientation propertiesHigh shrinkVery good tra.. |
|||
Tear Strength | 65.0 kN/m | 371 pli | Trouser Tear resistance MD; ISO 6383-1 |
EMS-Grivory Grivory® CR 8 PA* Product description: Grilon CR 8 is a Copolyamide. Grilon CR 8 shows the following features: High flexibility and toughnessGood thermoforming and orientation propertiesHigh shrinkageGood transparen.. |
|||
Tear Strength | 65.0 kN/m | 371 pli | Trouser Tear resistance TD; ISO 6383-1 |
EMS-Grivory Grivory® CR 8 PA* Product description: Grilon CR 8 is a Copolyamide. Grilon CR 8 shows the following features: High flexibility and toughnessGood thermoforming and orientation propertiesHigh shrinkageGood transparen.. |
|||
Tear Strength | 65.0 kN/m | 371 pli | Trouser Tear resistance MD; ISO 6383-1 |
EMS-Grivory Grivory® CR 9 HV PA* Product description: Grilon CR 9 HV is a high viscosity copolyamide with low temperature. Grilon CR9 HV has the following features:High flexibility and toughnessGood thermoforming and orientation pr.. |
|||
Tear Strength | 65.0 kN/m | 371 pli | Trouser Tear resistance TD; ISO 6383-1 |
EMS-Grivory Grivory® CR 9 HV PA* Product description: Grilon CR 9 HV is a high viscosity copolyamide with low temperature. Grilon CR9 HV has the following features:High flexibility and toughnessGood thermoforming and orientation pr.. |
|||
Tear Strength | 65.0 kN/m | 371 pli | Trouser Tear resistance MD; ISO 6383-1 |
EMS-Grivory Grivory® CR 9 PA* Product description: Grilon CR 9 is a copolyamide with low melting temperature. Grilon CR 9 shows the following features: High flexibility and toughnessGood thermoforming and orientation propertiesH.. |
|||
Tear Strength | 65.0 kN/m | 371 pli | Trouser Tear resistance TD; ISO 6383-1 |
EMS-Grivory Grivory® CR 9 PA* Product description: Grilon CR 9 is a copolyamide with low melting temperature. Grilon CR 9 shows the following features: High flexibility and toughnessGood thermoforming and orientation propertiesH.. |
|||
Tear Strength | 65.0 kN/m | 371 pli | Trouser Tear resistance MD; ISO 6383-1 |
EMS-Grivory Grivory® CA 6 E PA* Product description: Grilon CA 6 E is a non-extracted copolyamide with a low melting point. Grilon CA 6 E characterizes itself through the following properties Very high flexibility and toughnessVer.. |
|||
Tear Strength | 65.0 kN/m | 371 pli | Trouser Tear resistance TD; ISO 6383-1 |
EMS-Grivory Grivory® CA 6 E PA* Product description: Grilon CA 6 E is a non-extracted copolyamide with a low melting point. Grilon CA 6 E characterizes itself through the following properties Very high flexibility and toughnessVer.. |
|||
Tear Strength | 65.0 kN/m | 371 pli | ASTM D624 |
C.O.I.M. LARIPUR® LPR6515 Plasticized Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Tear Strength | 65.0 kN/m | 371 pli | ASTM D624 |
BASF Elastollan® C-70AW Polyester Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen.. |
|||
Tear Strength | >= 65.0 kN/m | >= 371 pli | ISO 34 |
Austin Novel Materials Texalan® 482A Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tear Strength | 65.0 kN/m | 371 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.0 PHR Thanecure ZM Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and man.. |
|||
Tear Strength | 65.1 kN/m | 371 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.75 PHR Zinc Stearate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 65.0 kN/m | 371 pli | 65 kN/m at 23°C. Value at 100°C is 36 kN/m. TPE-0056 (ASTM D 624) |
Advanced Elastomer Systems Santoprene® 283-40 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be .. |
|||
Tear Strength | >= 65.0 kN/m | >= 371 pli | ISO 34 |
Austin Novel Materials Texalan® 782A PCL TPU Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech |
|||
Tear Strength | 65.1 kN/m | 371 pli | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 65A Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |