Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 40.3 kN/m | 230 pli | ASTM D412 |
Multibase TPSiV™ 3011-50A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Tear Strength | 40.3 kN/m | 230 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Synprene™ RT-5180 RoHS Natural Styrene Butadiene Block Copolymer (SBC) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |
|||
Tear Strength | 40.3 kN/m | 230 pli | ASTM D624 |
PolyOne Versollan™ OM 1262NX-1 Thermoplastic Elastomer (TPE) Versollan™ OM 1262NX-1 is a performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS and PC/ABS substrates. - Excellent Grip with Matte, Rubbery Finish - Proven Track R.. |
|||
Tear Strength | 40.3 kN/m | 230 pli | ASTM D624 |
PolyOne Versollan™ OM 1262NX-9 Thermoplastic Elastomer (TPE) Versollan™ OM 1262NX-9 is a performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS, PC/ABS and copolyester substrates. - Excellent Grip with Matte, Rubbery Finish - P.. |
|||
Tear Strength | 40.3 kN/m | 230 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible A7000 Polyvinyl Chloride, Flexible (PVC, Flexible) Interior compound used primarily in transparent applications. This product is registered under UL 94 HB specifications @ 3.0 and 1.5 mm. thickness and all colors.Information provided by PolyOne |
|||
Tear Strength | 40.3 kN/m | 230 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible D75M0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 40.3 kN/m | 230 pli | ASTM D624 |
Multibase Multi-Flex® D 4210 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Noise DampingOzone Resistant Thermal Stability, GoodStiffness, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsInformation p.. |
|||
Tear Strength | 40.3 kN/m | 230 pli | Die B, post cured- 4 hours at 177°C; ASTM D624 |
Multibase C6-165 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 40.3 kN/m | 230 pli | Die B,molded-without post cure; ASTM D624 |
Multibase C6-265 DI-CUP R Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 40.3 kN/m | 230 pli | Die B,molded-without post cure; ASTM D624 |
Multibase C6-265 VAROX DBPH Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 40.3 kN/m | 230 pli | Die B,post cured- 2 hours at 177°C; ASTM D624 |
Multibase C6-265 VAROX DBPH Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 40.3 kN/m | 230 pli | ASTM D624 |
Multibase Multi-Flex® A 8103 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Heat StabilizedOzone ResistantGeneral Purpose Forms:PelletsProcessing Method:Injection MoldingBlow MoldingExtrusion Uses: Automotive Interior PartsInformation .. |
|||
Tear Strength | 40.3 kN/m | 230 pli | Fill/Transverse direction |
Saint-Gobain Chemlam® 3300 Multi-plied, Flexible, Non-porous Fluoropolymer Laminated Composite Description: Chemlam® Ultra® is the trademark for the Chemfab® family of multi-plied, flexible, non-porous fluoropolymer laminated composites that combine the feature of multi-layer fluorop.. |
|||
Tear Strength | 40.3 kN/m | 230 pli | Fill/Transverse direction |
Saint-Gobain Chemlam® 3320 High Mechanical Performance Industrial Laminate Description: Chemlam® Silver Ultra is the best mechanically performing series of Chemfab® industrial laminates. Chemlam® Silver Ultra composites feature uniform thickness, multi-layer cast .. |
|||
Tear Strength | 40.3 kN/m | 230 pli | Fill/Transverse direction |
Saint-Gobain Chemlam® 3320 Multi-plied, Flexible, Non-porous Fluoropolymer Laminated Composite Description: Chemlam® Ultra® is the trademark for the Chemfab® family of multi-plied, flexible, non-porous fluoropolymer laminated composites that combine the feature of multi-layer fluorop.. |
|||
Tear Strength | 40.3 kN/m | 230 pli | JIS K6301-B |
Stellarchem AB870EM TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Tear Strength | 40.3 kN/m | 230 pli | Fill/Transverse direction |
Saint-Gobain Chemlam® 3300 High Mechanical Performance Industrial Laminate Description: Chemlam® Silver Ultra is the best mechanically performing series of Chemfab® industrial laminates. Chemlam® Silver Ultra composites feature uniform thickness, multi-layer cast .. |
|||
Tear Strength | 40.3 kN/m | 230 pli | ASTM D624 |
Teknor Apex UNIPRENE® 7100-80 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tear Strength | 40.3 kN/m | 230 pli | Trouser; ASTM D470 |
Lubrizol ESTANE® ETE55DT3 Ester Based Thermoplastic Polyurethane Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, UV stableUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket.. |
|||
Tear Strength | 40.3 kN/m | 230 pli | Trouser; ASTM D470 |
Lubrizol ESTANE® ETE60DT3 Ester Based Thermoplastic Polyurethane Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, UV stableUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket.. |
|||
Tear Strength | 40.3 kN/m | 230 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 60A, Non-Black Peroxide Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 40.3 kN/m | 230 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 60A, Non-Black Peroxide Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 40.3 kN/m | 230 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® RT-3965 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerUV StabilizedNaturalApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionConsumer GoodsIndustrialProcessing Method:Injecti.. |
|||
Tear Strength | 40.3 kN/m | 230 pli | die B; ASTM D624 |
G-2703 Styrene-based Biomedical Elastomer |
|||
Tear Strength | 40.3 kN/m | 230 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® IT 584 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerOpaqueApplications:Multi-PurposeFDA (Food Contact)Processing Method:Injection MoldingPolyOne First ChoiceDisclaimer: A thermoplastic elas.. |