Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 43.8 kN/m | 250 pli | Die C; ASTM D624 |
Northstar Polymers MPP-A90A High Performance Polyether This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex.. |
|||
Tear Strength | 43.8 kN/m | 250 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible B7501 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 43.8 kN/m | 250 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible A7500 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Tear Strength | 43.8 kN/m | 250 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 64A MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 43.8 kN/m | 250 pli | ASTM D624 |
Multibase Multi-Flex® A 7041 Clear TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Tear Strength | 43.8 kN/m | 250 pli | ASTM D624 |
Multibase Multi-Flex® A 7802 TPE Blk Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Tear Strength | 43.8 kN/m | 250 pli | ASTM D624 |
Multibase Multi-Flex® A 8502 LC UV RXF/YYWA Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Tear Strength | 43.8 kN/m | 250 pli | Initial Tear Strength |
Saint-Gobain CHR® SG03-10(R) Premium Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 43.8 kN/m | 250 pli | Initial Tear Strength |
Saint-Gobain CHR® SG23-10(R) Primary Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 43.8 kN/m | 250 pli | Initial Tear Strength |
Saint-Gobain CHR® SG26-10(R) Primary Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 43.8 kN/m | 250 pli | Tensile Strength (Warp) |
Saint-Gobain Chemfab® 3790 Open Mesh Belting Description: General Notes on Saint Gobain Open Mesh Belting Products:CHEMFAB 1580, 1589 and 1590 are woven fiberglass belting materials designed for use in forced hot air curing ovens. Saint-Gobain.. |
|||
Tear Strength | 43.8 kN/m | 250 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® 13 Premium PTFE-Coated Glass Description: Chemfab® Premium Series combines a superior quality glass fabric with a high level of PTFE content. Description: Chemfab® Premium is an excellent multi-purpose fabric with a smoot.. |
|||
Tear Strength | 43.8 kN/m | 250 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® 13 Tear Resistant PTFE-Coated Glass Description: Chemfab® Tear Resistant Series is manufactured with specialized coating materials to improve tear and crease resistance. Uses for this series includes release sheets, belting and gas.. |
|||
Tear Strength | 43.8 kN/m | 250 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® 1580 PTFE Coated Fiberglass Conveyor Belting Description: General Notes on Saint Gobain Open Mesh Belting Products:CHEMFAB 1580, 1589 and 1590 are woven fiberglass belting materials designed for use in forced hot air curing ovens. Saint-Gobain.. |
|||
Tear Strength | 43.8 kN/m | 250 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 64A MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 43.8 kN/m | 250 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 65A MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | >= 43.8 kN/m | >= 250 pli | |
Arlon Thermavac® 0.060" (1.524 mm) Cured Silicone Vacuum Bagging (10502N060) Unsupported cured/post cured silicone rubber with a thickness of 0.060 in. ±0.006 (1.5 mm ±0.15 ); 0.003 in. (0.8 mm) polyethylene interleave. Color: Translucent. Weight: 2339 g/m² ± 234 (69.0.. |
|||
Tear Strength | >= 43.8 kN/m | >= 250 pli | |
Arlon Thermavac® 0.060" (1.524 mm) Cured Silicone Vacuum Bagging (10502R060) Unsupported cured/post cured silicone rubber with a thickness of 0.060 in. ±0.006 (1.5 mm ±0.15); 0.003 in. (0.8 mm) polyethylene interleave. The shelf life is defined as the duration of time for.. |
|||
Tear Strength | 43.8 kN/m | 250 pli | ASTM D624 |
ExxonMobil Santoprene® 8271-80HT Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic elastomer which complies with FDA regulations for rubber articles intended for repeated use. It can be processed using injection molding or extrusion melt pro.. |
|||
Tear Strength | 43.8 kN/m | 250 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® 14 High-Performance PTFE-Coated Glass Description: Chemfab® High-Performance Series provides the highest level of PTFE content for superior surface smoothness, durability, and longer life. Use this product for the most demanding heat s.. |
|||
Tear Strength | 43.8 kN/m | 250 pli | ASTM D624 |
Multibase Multi-Flex® A 8103 E Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection MoldingExtrusions Information provided by Multibase |
|||
Tear Strength | 43.8 kN/m | 250 pli | Die B, Silicone Property; ASTM D624 |
Arlon R36613N022 0.022" (0.559 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 7628 Heat Cleaned FiberglassSide 2: Cured Silicone RubberSide 2 Interleave: PolyethyleneFiberglas Weave: PlainThis data represents.. |